Development of hard intermetallic coatings on austenitic stainless steel by hot dipping in an Al-Si alloy
نویسندگان
چکیده
The austenitic stainless steel was coated by dipping into a molten Al-12.4%Si alloy at 765oC. The effect of immersion times in the range of 60 to 900 s was investigated with respect to the phase nature, thickness, and microhardness. An uniform layer (~12 m) of Al12(Fe,Cr)3Si2 intermetallic with hexagonal crystalline structure is formed, irrespectively the immersion time. Microhardness of the coating decreases with increasing dipping time, ranging between 850 and 600 HV for the shortest and longest immersion time, respectively. These hardness values are higher than that of about 200 HV for the substrate, which was not affected for the investigated periods of immersion.
منابع مشابه
Dissimilar laser welding of NiTi shape memory alloy to austenitic stainless steel archwires
In this research, dissimilar welding of NiTi shape memory alloy to AISI 304 austenitic stainless steel Archwires was investigated. For this purpose, common straight orthodontic archwire with rectangular cross-section and dimensions of (0.635 × 0.432 mm) were selected and the laser welding technique was used to connect the wires. The microstructure, chemical composition and phasesin the weld zon...
متن کاملDissimilar laser welding of NiTi shape memory alloy to austenitic stainless steel archwires
In this research, dissimilar welding of NiTi shape memory alloy to AISI 304 austenitic stainless steel Archwires was investigated. For this purpose, common straight orthodontic archwire with rectangular cross-section and dimensions of (0.635 × 0.432 mm) were selected and the laser welding technique was used to connect the wires. The microstructure, chemical composition and phasesin the weld zon...
متن کاملGrain Size Effect on the Hot Deformation Processing Map of AISI 304 Austenitic Stainless Steel
In this study, the hot deformation processing map of AISI 304 austenitic stainless steel in two initial grain sizes of 15 and 40 μm was investigated. For this purpose, cylindrical samples were used in the hot compression test at the temperature range of 950-1100 °C and the strain rate of 0.005-0.5% s-1. At first, the relationship between the peak stress and Zener-Hollomon parameter w...
متن کاملCorrosion Behavior of Detonation Gun Sprayed Fe-Al Type Intermetallic Coating
The detonation gun sprayed Fe-Al type coatings as an alternative for austenitic valve steel, were investigated using two different methods of testing corrosion resistance. High temperature, 10-hour isothermal oxidation experiments at 550, 750, 950 and 1100 °C show differences in the oxidation behavior of Fe-Al type coatings under air atmosphere. The oxide layer ensures satisfying oxidation resi...
متن کاملDevelopment of Alumina-Forming Austenitic Stainless Steels
This paper presents the results of the continued development of creep-resistant, alumina-forming austenitic (AFA) stainless steel alloys, which exhibit a unique combination of excellent oxidation resistance via protective alumina (Al2O3) scale formation and high-temperature creep strength through the formation of stable nano-scale MC carbides and intermetallic precipitates. Efforts in fiscal ye...