Variation of liquation cracking susceptibility for over–aged 247LC superalloy repair weld heat–affected zone

نویسندگان

چکیده

In this study, the liquation cracking temperature range (LCTR) of over-aged 247LC superalloy repair welds was quantitatively evaluated using spot-Varestraint testing, especially for application in weld heat-affected zone (HAZ). The metallurgical mechanism susceptibility and variation LCTRs superalloys clarified by analyzing microstructural characteristics at surface, thermodynamic calculations. From tests materials, LCTR to be 410 620 K 500 1000 h specimens, respectively. These results demonstrate that face significant serious HAZ. Based on local element distributions analyzed transmission electron microscopy Thermo-Calc calculations, underlying high overaged materials could attributed precipitation fine MC M6C carbides during over-aging treatment. promote interface between gamma phase temperatures lower than equilibrium solidus (1530 K) 247LC. estimated initiation MC/γ γ/M6C interfaces were 1125 1420 K,

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Evolution of Cast Microstructures on the HAZ Liquation Cracking of Mar-M004 Weld

The causes of liquation cracking in the heat-affected zone (HAZ) of a cast Mar-M004 superalloy weld were investigated. X-ray diffraction (XRD), electron probe microanalyzer (EPMA), and electron backscatter diffraction (EBSD) were applied to identify the final microconstituents at the solidification boundaries of the cast alloy. Fine borides and lamellar eutectics were present in front of some γ...

متن کامل

Liquation Cracking of Dissimilar Aluminum Alloys during Friction Stir Welding

A liquation cracking mechanism of dissimilar Al alloys during the friction stir welding (FSW) is suggested in this study. To identify the mechanism, the precipitates were analyzed and Al-Mg-Cu phase diagrams were calculated. Electron backscattering diffraction (EBSD) analysis and electron probe microanalysis (EPMA) were also conducted. In the same manner as constitutional liquation, at high hea...

متن کامل

Transgranular liquation cracking of grains in the semi-solid state

Grain refinement via semi-solid deformation is desired to obtain superior mechanical properties of cast components. Using quantitative in situ synchrotron X-ray tomographic microscopy, we show an additional mechanism for the reduction of grain size, via liquation assisted transgranular cracking of semi-solid globular microstructures. Here we perform localized indentation of Al-15wt.%Cu globular...

متن کامل

Research on the Grain Boundary Liquation Mechanism in Heat Affected Zones of Laser Forming Repaired K465 Nickel-Based Superalloy

The damaged K465 nickel-based superalloy parts were repaired by laser forming repair technology. The cracking characteristics and grain boundary liquation in heat affected zones were investigated by optical microscopy (OM), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). It was found that the cracks originated from the heat-affected zone and extended to the repai...

متن کامل

Analysis of Cracks in the Pulsed Nd:YAG Laser Welded Joint of Nickel-Based Superalloy

The weldability of GTD-111 nickel-based superalloy by pulsed Nd:YAG laser welding with an average power of 250 W was studied, and the microstructural evolution and cracking characteristics were also investigated. The solidification cracking of the fusion zone (FZ) and the intergranular liquation cracking in the heat affected zone (HAZ) were observed in the joint. Solidification cracking was cau...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Korean Journal of Metals and Materials

سال: 2023

ISSN: ['1738-8228', '2288-8241']

DOI: https://doi.org/10.3365/kjmm.2023.61.2.69