Tomographic Imaging of Bauxite Grains Leached Using Hydrochloric Acid

نویسندگان

چکیده

X-ray computer tomography (XRT) is a three-dimensional, nondestructive, and thus reproducible examination method that allows for the investigation of internal external structures objects. Due to its characteristics, XRT technique has increasingly established itself as an alternative also applied in field mineral processing. Within this work, used investigate influence hydrochloric acid leaching iron-rich bauxites on grain composition. Acid promising beneficiation refractories. Many studies have already with can reduce Fe2O3 content bauxites. However, apart from process composition bauxites, aspects such exact constitution or porosity behavior rarely been considered so far. To address these open questions, analysis was examine characterize various By comparing identical grains before after leaching, it observed gibbsite penetration deeper, volume decreases significantly. In diasporic boehmitic clear edges be seen which iron reduced.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Iron leaching from bauxite ore in hydrochloric acid using response surface methodology

In this work, hydrochloric acid is used to remove iron impurities in the bauxite ore contained in the diasporite mineral located in the Sari region. The bauxite ore was calcined at different temperatures and times, and then dissolved in a hydrochloric acid solution. After determining the optimum calcination conditions in 1 h at 900 °C, the response surface methodology (RSM) with four factors in...

متن کامل

Solvent Extraction of Gold from Hydrochloric Acid-Leached Nigerian Gold Ore by Tributylphosphate

This paper presents an experimental study on the dissolution kinetics and solvent extraction of total gold from Ijero-ekiti (Nigeria) gold ore deposit by hydrochloric acid leaching followed by extraction with Tributylphosphate (TBP) in kerosene. The leaching investigation showed that the gold ore dissolution in HCl solution increases with increasing acid concentration, temperature and with decr...

متن کامل

iron leaching from bauxite ore in hydrochloric acid using response surface methodology

in this work, hydrochloric acid is used to remove iron impurities in the bauxite ore contained in the diasporite mineral located in the sari region. the bauxite ore was calcined at different temperatures and times, and then dissolved in a hydrochloric acid solution. after determining the optimum calcination conditions in 1 h at 900 °c, the response surface methodology (rsm) with four factors in...

متن کامل

The Combination of Edestin with Hydrochloric Acid

Electromotive force measurements of cells without liquid junction, of the type Ag, AgCl, HCl + protein, H(2), lead to the conclusion that 1 gm. of edestin (or, more probably, edestan) combines with a maximum of 13.4 x 10(-4) equivalents of H(+) and 3.9 x 10(-4) equivalents of Cl(-), when the protein is dissolved in 0.1 M HCl.

متن کامل

Multidimensional Tomographic Imaging Using Volume Holography

We propose the application of volume holography to fourdimensional (4-D) spatiospectral imaging. The proposed systems use materials and techniques developed for holographic data storage and interconnections to capture three-dimensional (3-D) spatial and one-dimensional (1-D) spectral information about a remote light source or scatterer. We analyze case studies of simple architectures using sphe...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Minerals

سال: 2023

ISSN: ['2075-163X']

DOI: https://doi.org/10.3390/min13070884