TLP Weldability of Nickel-Base Superalloys

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Review on Thermo-Mechanical Fatigue Behavior of Nickel-Base Superalloys

Nickel-base superalloys have become the key materials of hot-end components in the aeroengines over the past several decades. Nickelbase superalloys are easy to produce thermo-mechanical fatigue (TMF) behavior when withstanding the combined effects of high temperature, creep, oxidation, mechanical stress and thermal stress. The occurrence of TMF seriously affects the normal service for hot-end ...

متن کامل

Residual Stress Assessment in Surface-treated Nickel-base Superalloys

Experimental results are presented to illustrate that there exists a unique window of opportunity for eddy current NDE of residual stress in surface-treated nickel-base superalloys. In light of its frequency-dependent penetration depth, the measurement of eddy current conductivity has been suggested as a possible means to allow the nondestructive evaluation of subsurface residual stresses in su...

متن کامل

Strain induced abnormal grain growth in nickel base superalloys

Under certain circumstances abnormal grain growth occurs in Nickel base superalloys during thermomechanical forming. Second phase particles are involved in the phenomenon, since they obviously do not hinder the motion of some boundaries, but the key parameter is here the stored energy difference between adjacent grains. It induces an additional driving force for grain boundary migration that ma...

متن کامل

Effect of bonding time on microstructure and mechanical properties during TLP bonding of nickel-base superalloys Hastelloy C276 and Stainless Steel AISI316

Joining of Hastelloy C276 nickel-base superalloy to AISI316 Stainless Steel using BNi-2 interlayer performed by transient liquid phase process (TLP) at 1150°C for 5 and 30 minutes. Bonding microstructure was studied using an Optical microscope and a scanning electron microscope (SEM). Vickers hardness test and shear strength test have been used to evaluate the mechanical properties. Microstruct...

متن کامل

Effect of bonding time on microstructure and mechanical properties during TLP bonding of nickel-base superalloys Hastelloy C276 and Stainless Steel AISI316

Joining of Hastelloy C276 nickel-base superalloy to AISI316 Stainless Steel using BNi-2 interlayer performed by transient liquid phase process (TLP) at 1150°C for 5 and 30 minutes. Bonding microstructure was studied using an Optical microscope and a scanning electron microscope (SEM). Vickers hardness test and shear strength test have been used to evaluate the mechanical properties. Microstruct...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Japan Welding Society

سال: 1980

ISSN: 0021-4787,1883-7204

DOI: 10.2207/qjjws1943.49.462