Thermal, Metallurgical and Mechanical Determinants of Laminar Nickel/Aluminum Dissimilar Alloys during Laser-material Interaction Part I: Nickel-based Superalloy

نویسندگان

چکیده

To develop in-depth understanding of metallurgical phenomena for completeness, mechanical heterogeneity is kinetically and thermodynamically explained by thorough microstructure characterization engineering materials, e.g. polycrystalline nickel-based superalloy, alleviation weldability-related problems during laser-induced keyhole fabrication. Because nonequilibrium solidification behavior inside weld pool, finer γ phase dendrite substructure confined to partition-resistant bottom part, coarser crystallography-independently circumscribed at partition-vulnerable neck transition region full penetration weld, thus lack homogeneity. Abundance segregation-driven eutectic or intermetallic in the interdendrite area throughout essentially attributable conditions, morphologically increases susceptibility properties deterioration. As a result instability, Niobium-aided Laves/γ reaction vicinity interstices terminal stage contributes severe boundaries brittleness, impairs properties, which consistent with metallography fractography results, more deleterious weldability, since solute redistribution supersaturation adversely exacerbate segregation residual liquid, especially asymmetric pool shape. There inverse parabolic relationship between secondary arm spacing partition coefficient, when location varies from nail-shaped upper site site. Chemical, microstructural heterogeneities are geometrically favorable curvature-related region. In addition, mechanism thermal, inhomogeneities, attributed shape, consequently proposed. Untoward phenomena, such as brittle Niobium-rich phases mitigate strength, ductility toughness weld. order macroscopically microscopically satisfy superior requirement, chemistry high quality metallurgically controlled. Fruitful information data further support reasonable explanations. It imperative progressively advance welding metallurgy, weldability fabricability intricate shape defects minimization, suppress through viable design control laser processing, simultaneously.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Laser welding of dissimilar aluminium alloys with filler material

Laser welding of dissimilar aluminium alloys with filler material Luís Filipe Amaro Pinto Instituto Superior Técnico – Technical University of Lisbon – Portugal September 2008 Abstract The aluminium alloys are materials with great potential because of its high strength and low weight. However, the welding of dissimilar aluminium alloys is difficult in autogeneous welding, due to these alloys ar...

متن کامل

Mechanical and Metallurgical Aspects of Dissimilar Metal Welds a Review

A literature review of studies and researches has been attempted in the field of dissimilar metal welding. Dissimilar metal welds have numerous industrial applications in area of thermal power generation, chemical, petrochemical, automobile, aerospace industries and nuclear plants etc. The purpose of this paper is to review: (a) Dissimilar metal welds, their Metallurgical and Mechanical aspects...

متن کامل

Constitutive Model Based on Dynamic Recrystallization Behavior during Thermal Deformation of a Nickel-Based Superalloy

Peng Zhang 1, Cen Yi 1, Gang Chen 1, Heyong Qin 2 and Chuanjie Wang 1,* 1 School of Materials Science and Engineering, Harbin Institute of Technology at Weihai, Weihai 264209, China; [email protected] (P.Z.); [email protected] (C.Y.); [email protected] (G.C.) 2 Central Iron & Steel Research Institute, Beijing 100081, China; [email protected] * Correspondence: [email protected]; Tel.: +86-631-568...

متن کامل

Laser Cladding of Ultra-Thin Nickel-Based Superalloy Sheets

Laser cladding is a well-established process to apply coatings on metals. However, on substrates considerably thinner than 1 mm it is only rarely described in the literature. In this work 200 µm thin sheets of nickel-based superalloy 718 are coated with a powder of a cobalt-based alloy, Co-28Cr-9W-1.5Si, by laser cladding. The process window is very narrow, therefore, a precisely controlled Yb ...

متن کامل

Analysis of Cracks in the Pulsed Nd:YAG Laser Welded Joint of Nickel-Based Superalloy

The weldability of GTD-111 nickel-based superalloy by pulsed Nd:YAG laser welding with an average power of 250 W was studied, and the microstructural evolution and cracking characteristics were also investigated. The solidification cracking of the fusion zone (FZ) and the intergranular liquation cracking in the heat affected zone (HAZ) were observed in the joint. Solidification cracking was cau...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of physics

سال: 2022

ISSN: ['0022-3700', '1747-3721', '0368-3508', '1747-3713']

DOI: https://doi.org/10.1088/1742-6596/2348/1/012001