Thermal degradation studies of several pyrrone films
نویسندگان
چکیده
منابع مشابه
Control of Several Emissions during Olive Pomace Thermal Degradation
Biomass plays an important role as an energy source, being an interesting alternative to fossil fuels due to its environment-friendly and sustainable characteristics. However, due to the exposure of customers to emissions during biomass heating, evolved pollutants should be taken into account and controlled. Changing raw materials or mixing them with another less pollutant biomass could be a su...
متن کاملEffect of Fe3+–MMT on thermal degradation and mechanical behavior of PVP/Amylose nanocomposite films
Novel nanocomposite films based on amylose (AM) and Fe3+-montmorillonite (Fe3+–MMT) in the matrix of poly (vinyl pyrrolidone) (PVP) were fabricated by using a solution casting method. The X-Ray diffractional analysis indicated that an ion-exchange process occurred between Fe3+–MMT and PVP. Thermogravimetrical analysis (TGA), differential termogravivetrical analy...
متن کاملSynthesis and Thermal Degradation Studies of Melamine Formaldehyde Resins
Melamine formaldehyde (MF) resins have been synthesized at different reaction temperature and pH values. Different molar ratios of melamine and formaldehyde were used to synthesize the corresponding resins. The prepared resin samples were characterized by using molecular weight determination viscometry and thermogravimetric analysis (TGA). The maximum percentage of solid content (69.7%) was obt...
متن کاملChitosan/Poly(Amide-Imide) Blend Films: Studies on Thermal and Mechanical Stability, Morphology and Biodegradability
A diacid monomer was synthesized by the condensation of L-tryptophan amino acid and pyromellitic dianhydride (PMDA). The diacid was utilized for the synthesis of three types of poly(amide-imide)s (PAIs) using three different kinds of diamines. The synthesized monomer and PAIs were characterized using FT-IR, 1H-NMR and 13C-NMR spectroscopies and the PAIs were also used ...
متن کاملThermal Degradation
When wood is exposed to elevated temperatures, changes can occur in its chemical structure that affect its performance. The extent of the changes depends on the temperature level and the length of time under exposure conditions. The changes in chemical structure may be manifested only as reduced strength, and hydroscopic water and volatile oil weight loss. In contrast, very drastic chemical cha...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Applied Polymer Science
سال: 1968
ISSN: 0021-8995,1097-4628