Thermal annealing of sequentially deposited SnS thin films
نویسندگان
چکیده
منابع مشابه
Thermal Annealing Influence over Optical Properties of Thermally Evaporated SnS/CdS Bilayer Thin Films
Thin films of tin sulfide/cadmium sulfide (SnS/CdS) were prepared bythermal evaporation method at room temperature on a glass substrate and then annealedat different temperature with the aim of optimizing the optical properties of the materialfor use in photovoltaic solar cell devices. The effect of annealing on optical propertiesof SnS/CdS film was studied in the temper...
متن کاملThe effects of thermal annealing on the obliquely deposited Ag–Ge–S thin films
Obliquely deposited thin films of ternary Ag–Ge–S glasses are characterized in this work. Thin films are fabricated in a vacuum thermal evaporator at different evaporation angles and examined by Raman spectroscopy. The Raman mode frequency of GeS4 corner-sharing (CS) structure of the as-deposited films display a red-shift as a function of Ag content due to reduced global connectivity, and there...
متن کاملEnhanced methanol sensing performance of oblique deposited WO3 thin films
Methanol (CH3OH) is a colorless liquid with a mild odor. The wide ranges of applications, toxicity and clinical implications of methanol have made necessary to develop reliable and high-performance methanol sensors. In this paper, WO3 thin films were deposited on SiO2/Si substrates by e-beam evaporation technique under normal and oblique angles and then post-annealed at 500 °C with a flow of ox...
متن کاملStudy of Aluminum Oxide Films Deposited using Thermal ALD and Effect of Low Thermal Budget Annealing
Thermal ALD deposited Al2O3 films on silicon show marked difference in surface passivation quality as a function of annealing time (using rapid thermal process). An effective and quality passivation is realized in short anneal duration (~100s) which is reflected in the low surface recombination velocity (SRV <10 cm/s). The deduced values are close to the best reported SRV obtained by high therm...
متن کاملInfluence of Deposition Time on Structural and Optical Properties of Chemically Deposited SnS Thin Films
Using chemical bath deposition (CBD) technique SnS thin films have been deposited at room temperature with different deposition times. The deposited films have been investigated through Xray diffraction measurements to determine structural properties. The deposited SnS films found amorphous and polycrystalline with an orthorhombic herzenbergite structure. The grain size found to increase with d...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Proceedings of the Estonian Academy of Sciences
سال: 2015
ISSN: 1736-6046
DOI: 10.3176/proc.2015.4.04