The effect of surface preparation on the protective properties of Al2O3 and HfO2 thin films deposited on cp-titanium by atomic layer deposition

نویسندگان

چکیده

Atomic layer deposition (ALD), a method that allows the formation of thin and conformal films on substrates interest, was employed to prepare alumina (Al2O3) hafnia (HfO2), with aim protecting surface commercially pure titanium (cp-Ti) used in biomedical applications. Prior deposition, cp-Ti specimens have been prepared two ways – grinding followed by polishing. Such surfaces denoted as rough smooth, respectively. The thickness, composition, morphology topography determined using ellipsometry, focused ion beam microscopy energy dispersive X-ray spectroscopy, time-of-flight secondary mass spectrometry 3D profilometry. A homogeneous stoichiometric composition obtained thickness ca. 150 nm. anti-corrosive properties ALD were measured simulated body fluid solution, electrochemical impedance spectroscopy (EIS) potentiodynamic polarization curves. roughness plays an important role protective these films, especially those hafnia. In general, when deposited smooth surface, better obtained, evidenced EIS long-term, 40-day tests. showed very low porosity, calculated from parameters, significantly lower corrosion current densities, compared bare specimens. Lower porosity slightly provided On other hand, according long-term tests, retained greater values than Since both are biocompatible materials, this study confirms possibility their use reduce risk failure medical implants made cp-Ti, human environment.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Surface Passivation of Silicon Using HfO2 Thin Films Deposited by Remote Plasma Atomic Layer Deposition System

Hafnium oxide (HfO2) thin films have attracted much attention owing to their usefulness in equivalent oxide thickness scaling in microelectronics, which arises from their high dielectric constant and thermodynamic stability with silicon. However, the surface passivation properties of such films, particularly on crystalline silicon (c-Si), have rarely been reported upon. In this study, the HfO2 ...

متن کامل

Effects of Al Doping on the Properties of ZnO Thin Films Deposited by Atomic Layer Deposition

The tuning of structural, optical, and electrical properties of Al-doped ZnO films deposited by atomic layer deposition technique is reported in this work. With the increasing Al doping level, the evolution from (002) to (100) diffraction peaks indicates the change in growth mode of ZnO films. Spectroscopic ellipsometry has been applied to study the thickness, optical constants, and band gap of...

متن کامل

the washback effect of discretepoint vs. integrative tests on the retention of content in knowledge tests

در این پایان نامه تاثیر دو نوع تست جزیی نگر و کلی نگر بر به یادسپاری محتوا ارزیابی شده که نتایج نشان دهندهکارایی تستهای کلی نگر بیشتر از سایر آزمونها است

15 صفحه اول

the effect of taftan pozzolan on the compressive strength of concrete in the environmental conditions of oman sea (chabahar port)

cement is an essential ingredient in the concrete buildings. for production of cement considerable amount of fossil fuel and electrical energy is consumed. on the other hand for generating one tone of portland cement, nearly one ton of carbon dioxide is released. it shows that 7 percent of the total released carbon dioxide in the world relates to the cement industry. considering ecological issu...

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Electrochimica Acta

سال: 2021

ISSN: ['1873-3859', '0013-4686']

DOI: https://doi.org/10.1016/j.electacta.2020.137431