The Effect of Deposition Temperature of TiN Thin Film Deposition Using Thermal Atomic Layer Deposition
نویسندگان
چکیده
In this study, the effect of deposition temperature TiN thin films deposited using thermal atomic layer (ALD) method was investigated. TiCl4 precursor and NH3 reactive gas were used, rate, resistivity change, surface morphology characteristics compared in range 400 °C–600 °C. While decreased to 177 µΩcm as increased 600 °C, an increase roughness (Rq) 0.69 nm a deterioration step coverage identified. order obtain high-quality film with excellent even at low temperatures, post-treated plasma combination N2/He ratio 3:2 confirm change resistivity. X-ray diffraction analysis confirmed crystallization caused by energy. As result, °C be lowered about 25%.
منابع مشابه
Atomic Layer Deposition of Tin Monosulfide Thin Films
Thin film solar cells made from earth-abundant, non-toxic materials are needed to replace the current technology that uses Cu(In,Ga)(S,Se)2 and CdTe, which contain scarce and toxic elements. One promising candidate absorber material is tin monosulfide (SnS). In this report, pure, stoichiometric, single-phase SnS films were obtained by atomic layer deposition (ALD) using the reaction of bis(N,N’...
متن کاملLow Temperature Atomic Layer Deposition of Tin Oxide
Atomic layer deposition (ALD) of tin oxide (SnOx) films was achieved using a newly synthesized tin precursor and hydrogen peroxide. We obtained highly pure, conductive SnOx films at temperatures as low as 50 C, which was possible because of high chemical reactivity between the new Sn precursor and hydrogen peroxide. The growth per cycle is around 0.18 nm/cycle in the ALDwindow up to 150 C, and ...
متن کاملAtomic layer deposition (ALD): from precursors to thin film structures
The principles of the atomic layer deposition (ALD) method are presented emphasizing the importance of precursor and surface chemistry. With a proper adjustment of the experimental conditions, i.e. temperatures and pulsing times, the growth proceeds via saturative steps. Selected recent ALD processes developed for films used in microelectronics are described as examples. These include depositio...
متن کاملLow-temperature thin-film deposition and crystallization.
Crystalline oxide films are important components in a wide array of electronic and optical devices, and their study and manufacture involve major aspects of current science and technology. A plethora of methods, such as sputtering, chemical vapor deposition, pulsed laser deposition, and sol-gel, are commonly used to deposit these films, and many new techniques are being developed (1). In each o...
متن کاملSurface chemistry and film growth during TiN atomic layer deposition 4 using TDMAT and NH 3
22 Abstract 23 24 Surface chemistry and film growth were examined during titanium nitride (TiN) atomic layer deposition (ALD) using sequential 25 exposures of tetrakis-dimethylamino titanium (TDMAT) and NH . This ALD system is shown to be far from ideal and illustrates 3 26 many potential problems that may affect ALD processing. These studies were performed using in situ Fourier transform infra...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Coatings
سال: 2023
ISSN: ['2079-6412']
DOI: https://doi.org/10.3390/coatings13010104