Study on Variable Stress Corrosion Susceptibility of Four Typical High-Strength Sucker Rods in High-Salinity Well Fluids

نویسندگان

چکیده

To study the corrosion characteristics of high-strength sucker rods in high-salinity well fluids under alternating stresses, a single-factor stress test was designed. The slow strain rate tensile (SSRT) carried out for four kinds different Cl− and HCO3− concentrations with service strengths, variable cracking susceptibility analyzed. results show that elongation loss absorbed work H-grade ultra-high-strength 4330 rod after are greater than those both 4142 20CrMoA rod. 30CrMoA less affected by changes HCO3−. With increase use strength, increase. change surface during process is inconsistent actual loss. It can be concluded not necessarily related to strength suitable applications wells high concentration Cl−, but it operation alkaline conditions where corrosive media such as coexist. Under highly mineralized conditions, susceptible corrosion. lower In fluids, higher is. weight-loss-based plastic may contradict determination material working conditions.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

focus on communication in iranian high school language classes: a study of the role of teaching materials in changing the focus onto communication in language classes

چکیده ارتباط در کلاس به عوامل زیادی از جمله معلمان، دانش آموزان، برنامه های درسی و از همه مهم تر، مواد آموزشی وابسته است. در تدریس ارتباطی زبان که تاکید زیادی بر توانش ارتباطی دارد، کتاب درسی به عنوان عامل موثر بر پویایی کلاس محسوب میگردد که درس ها را از طریق فراهم آوردن متن ارتباط کلاسی و هم چنین نوع تمرین زبانی که دانش آموزان در طول فعالیت های کلاسی به آن مشغول اند، کنترل می کند. این حقیقت ک...

15 صفحه اول

Stress- Corrosion Crack Initiation of High-strength Pipeline Steel in Near-neutral pH Environments

Stress-corrosion cracking (SCC) tests were conducted in the near-neutral pH standard solution, NS4, and in an actual soil solution, using four-point bending at a high stress ratio and low frequency conditions very similar to those of operational pipelines. Pitting incubation appeared first and then pitting initiated and grew in both solutions although there were many more pits on the specimen t...

متن کامل

High Strength Corrosion Resistant Metals

There are a number of ways to improve the corrosion and abrasion resistance of metals, including alloying, anodizing, nitriding and application of protective thin films. Alloying involves generating a binary phase diagram to determine the optimum composition and temperature dependence. For example, copper alloys known as “bronzes” offer high strength, abrasion resistance and high temperature co...

متن کامل

Strength Sucker Rod Steel in High SO42- Environment

9 In some sour reservoirs and tertiary oil recovery blocks, SO42in solution can cause the corrosion 10 and corrosion fatigue of the sucker rods. In this paper, the corrosion behaviors of super-strength 11 sucker rod FG20 (16Mn2SiCrMoVTiA) steel in the well fluid are investigated by electrochemical 12 measurements, and electron probe micro-analyzer (EPMA) analysis. The results show that FG20 ste...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Processes

سال: 2023

ISSN: ['2227-9717']

DOI: https://doi.org/10.3390/pr11092762