Micro texture tools (MTTs) with variable distribution density were proposed, and the novel MTTs can adapt to different friction states in tool chip contact area maintain good anti-friction wear resistance. The composed of two regions groove width which prepared on rake face by femtosecond laser technology. cutting processes carried out turning superalloy GH4202. According machining characteristics (rake wear, volume, workpiece material adhesion morphology), role was analyzed. experimental results showed that parameters region near away from edge have effects mechanisms characteristics. Compared a non-textured uniform textured tool, proper design make better resistance breaking ability when
منابع مشابه
Hard turning with variable micro-geometry PcBN tools
This paper presents investigations on hard turning with variable edge design PcBN inserts. Turning of hardened AISI 4340 steel with uniform and variable edge design PcBN inserts is conducted, forces and tool wear are measured. 3D finite element modelling is utilized to predict chip formation, forces, temperatures and tool wear on uniform and variable edge micro-geometry tools. Predicted forces ...
متن کاملMicro Wire Electrical Discharge Machining , Main Aspects , Tools And
The increasing demand of micro or miniature parts and the development of the micro machining processes are the cause of the growing of micro wire electrical discharge machining (μ-WEDM). μ-WEDM has the ability to manufacture complicate shapes with high accuracy and provides the advantage of machining any conductive materials regardless of their mechanical properties in the absence of significan...
متن کاملPhysics-Embedded Machine Learning: Case Study with Electrochemical Micro-Machining
Although intelligent machine learning techniques have been used for input-output modeling of many different manufacturing processes, these techniques map directly from the input process parameters to the outputs and do not take into consideration any partial knowledge available about the mechanisms and physics of the process. In this paper, a new approach is presented for taking advantage of th...
متن کاملMachining Response in Turning Aluminium Composite LM13 With 15% SiC
In this paper, an attempt has been made to experimental investigation the machinability of aluminum metal matrix composite (LM13/SiC/15p) during continuous turning of composite rods using carbide inserts. Base matrix material is Aluminium LM13 reinforced with 15 % weight by volume of Silicon carbide particles of mean diameter 20 μm to 40 μm is used. The main focus of investigation is to determi...
متن کاملEvaluation of Tool Performance With Nanocrystalline Multilayer Coatings on the Machinability of Superalloy Inconel 718
In this paper, the performance of the cutting tool with nanocrystalline multilayer coatings (TiN+TiAlN) for machining of superalloy Inconel 718 in the dry and wet conditions was studied. The multi layer TiN and TiAlN with nanocrystalline structure was applied by physical vapor deposition technique (arc evaporation) on the WC-Co inserts. The results of the ball on disc wear test and the machinin...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: The International Journal of Advanced Manufacturing Technology
سال: 2022
ISSN: ['1433-3015', '0268-3768']
DOI: https://doi.org/10.1007/s00170-022-10117-2