Study of Temper Embrittlement in HAZ of Cr-Mo Steels (Report 4). Temper Embrittlement in HAZ of 2 1/4Cr-1Mo Steel Induced by Reheating after SR Treatment.
نویسندگان
چکیده
منابع مشابه
Study on Temper Embrittlement and Hydrogen Embrittlement of a Hydrogenation Reactor by Small Punch Test
The study on temper embrittlement and hydrogen embrittlement of a test block from a 3Cr1Mo1/4V hydrogenation reactor after ten years of service was carried out by small punch test (SPT) at different temperatures. The SPT fracture energy Esp (derived from integrating the load-displacement curve) divided by the maximum load (Fm) of SPT was used to fit the Esp/Fm versus-temperature curve to determ...
متن کاملOn the Step Cooling Treatment for the Assessment of Temper Embrittlement Susceptibility of Heavy Forgings in Superclean Steels
When subjected to extended exposure to intermediate service temperatures, Cr–Mo steels, Ni–Cr steels, and 5% Ni steels can become embrittled, with an associated decrease in fracture toughness and a shift in the ductile-to-brittle transition temperature to higher temperatures. Two methods for the investigation of temper embrittlement phenomena are isothermal aging or the use of a step cooling ag...
متن کاملstudy of cohesive devices in the textbook of english for the students of apsychology by rastegarpour
this study investigates the cohesive devices used in the textbook of english for the students of psychology. the research questions and hypotheses in the present study are based on what frequency and distribution of grammatical and lexical cohesive devices are. then, to answer the questions all grammatical and lexical cohesive devices in reading comprehension passages from 6 units of 21units th...
Charpy Notch Toughness and Hardness of Reheated Martensite and Lower Bainite
The resistance to hydrogen embrittlement is of essential importance for steels for vessels for storage of hydrocarbons and depends on the effect of absorbed hydrogen on steel ductility. API tests have shown for the 490 MPa yield stress HSLA steels with the microstructure of ferrite and cementite particles a much greater reduction of area than for the 350 MPa steel with the microstructure of pol...
متن کاملPrevention of Hydrogen Embrittlement in Steels
The essential facts about the nature of the hydrogen embrittlement of steels have now been known for 140 years. It is diffusible hydrogen that is harmful to the toughness of iron. It follows, therefore, that the harmful influence of diffusible hydrogen can be mitigated by preventing its entry into steel or by rendering it immobile once it penetrates the material. This review deals with the meth...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY
سال: 1998
ISSN: 0288-4771
DOI: 10.2207/qjjws.16.243