Stress-dependent adhesion and sliding-induced nanoscale wear of diamond-like carbon studied using in situ TEM nanoindentation

نویسندگان

چکیده

We present the first in situ transmission electron microscope (TEM) study of extended sliding diamond-like carbon (DLC) on diamond. show how tribological properties amorphous (a-C) reach their limit by exploring onset wear for harsh condition against diamond vacuum. A particularly hard, hydrogen-free member DLC family, a-C is wide technological interest, but mechanisms which damage occurs during contact are not well understood. Real-time TEM imaging nanoscale area provides insight into and damage. that at high normal stresses with full contributing to additional shear stress, initially low adhesion a-C-diamond interface rapidly increases a rate greater than seen similar silicon-diamond studies. propose away relatively surface energy sp2-rich layer outer surface, exposing sp3-rich sub-layers can form covalent bonds require more tensile force be broken, leading higher an acceleration wear.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Nanoscale Abrasive Wear of CoCrMo in In Situ TEM Sliding

The mechanical behaviour of materials at nanometre dimensions has been a major recent topic of research. In this study, the wear properties of a *60-nm thin foil made of the ductile fcc phase of a CoCrMo alloy were examined using in situ sliding test in a transmission electron microscope by sliding a silicon AFM tip on the fcc matrix under an applied normal load of 416–1,279 nN. The material ne...

متن کامل

Voltage assisted asymmetric nanoscale wear on ultra-smooth diamond like carbon thin films at high sliding speeds

The understanding of tribo- and electro-chemical phenomenons on the molecular level at a sliding interface is a field of growing interest. Fundamental chemical and physical insights of sliding surfaces are crucial for understanding wear at an interface, particularly for nano or micro scale devices operating at high sliding speeds. A complete investigation of the electrochemical effects on high ...

متن کامل

In situ TEM nanoindentation of nanoparticles.

The deformation behavior of nanoparticles continues to be an exciting area for materials research. Typically, nanoparticles show a conspicuous lack of dislocations, even after significant deformation. Therefore, it has been suggested that dislocations cannot exist or/do not play a role on the deformation of nanoparticles. In situ TEM nanoindentation is a critical tool for addressing this issue ...

متن کامل

Ultralow nanoscale wear through atom-by-atom attrition in silicon-containing diamond-like carbon.

Understanding friction and wear at the nanoscale is important for many applications that involve nanoscale components sliding on a surface, such as nanolithography, nanometrology and nanomanufacturing. Defects, cracks and other phenomena that influence material strength and wear at macroscopic scales are less important at the nanoscale, which is why nanowires can, for example, show higher stren...

متن کامل

The Wear Resistance of Cryogenically Treated Diamond-Like Carbon Films

This study explored the effects of cryogenic treatment on the microstructure, hardness, and wear-resistance of diamond-like carbon (DLC) by cryogenically treating NAK 80 mold steel coated with DLC. Raman spectroscopy analyzed the structure of the DLC film. Nanoindenter analyzed the hardness and Young’s modulus of the film, and their relationship determined the wear resistance. Wear test assesse...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Carbon

سال: 2022

ISSN: ['0008-6223', '1873-3891']

DOI: https://doi.org/10.1016/j.carbon.2022.03.030