Solid-State Joining of Dissimilar Ni-Based Superalloys via Field-Assisted Sintering Technology for Turbine Applications

نویسندگان

چکیده

Friction welding or electron/laser beam of nickel superalloys compromises the microstructure with localized melting and heat-affected zones (HAZ). In this work, Field-Assisted Sintering Technology (FAST) is studied as an alternative method for solid-state diffusion bonding CM247LC Inconel 718. Bonding microstructures room-temperature tensile strengths are evaluated. Preliminary results suggest that FAST leads to interface a compositional gradient without producing HAZ losing strength.

منابع مشابه

Using Solid-State Joining in Gas Turbine Engines

$1.00 TO ASME MEMBERS The Society shall not be responsible for statements or opinions advanced in papers or in discussion at meetings of the Society or of its Divisions or Sections, or printed in its publications. Discussion is printed only if the paper is published in an ASME journal or Proceedings. Released for general publication upon presentation. Full credit should be given to ASME, the Pr...

متن کامل

MODELLING THE MATERIAL PROPERTIES AND BEHAVIOUR OF Ni-BASED SUPERALLOYS

At the last two Superalloy meetings at Seven Springs, work on the development of thermodynamic modelling tools for application to multi-component Ni-based superalloys has been presented. Such modelling has become quite widespread, providing significant benefit. However, its applicability often falls short from directly providing the information that is actually required and, by itself, cannot b...

متن کامل

Novel Titanium Manganese Alloys and Their Macroporous Foams for Biomedical Applications Prepared by Field Assisted Sintering

In this chapter, a novel titanium (Ti) alloy and foam suitable for biomedical applications will be introduced. As we know, Ti and its alloys are widely used as biomaterials especially for orthopedic implants in load bearing sites as dental and orthopedic implants and heart valves, due to their high mechanical properties, corrosion resistance and biocompatibility (Geetha et al., 2009). Pure Ti w...

متن کامل

High Temperature Nanoindentation of Ni-base Superalloys

Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metallurgical and Materials Transactions

سال: 2021

ISSN: ['1073-5623', '1543-1940']

DOI: https://doi.org/10.1007/s11661-021-06274-w