Slurry Erosion Characteristics of Stellite 6 on AISI 316 and AISI 410 Stainless Steels

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Mechanical Properties of Boronized AISI 316, AISI 1040, AISI 1045 and AISI 4140 Steels

In this study, some mechanical properties of borided and unborided four steels were investigated. Boronizing of steels was performed by powder pack method at 1210 K for 4 h. The hardness of borides, boride layer thickness and room temperature tensile properties were measured and it was observed that hardness and tensile properties strongly depend on chemical composition of steels. In addition, ...

متن کامل

Dynamic Strain Ageing and Eac of Deformed Nitrogen-alloyed Aisi 316 Stainless Steels

Intergranular stress corrosion cracking has occurred in BWR environments in non-sensitised, cold-worked austenitic stainless steel materials. The affecting parameters are so far not fully known, but deformation mechanisms may be decisive. The effect of cold deformation and nitrogen content on the deformation behaviour of austenitic stainless steels was investigated. The materials were austeniti...

متن کامل

Corrosion and microstructural analysis data for AISI 316L and AISI 347H stainless steels after exposure to a supercritical water environment.

This article presents corrosion data and microstructural analysis data of austenitic stainless steels AISI 316L and AISI 347H exposed to supercritical water (25 MPa, 550 °C) with 2000 ppb of dissolved oxygen. The corrosion tests lasted a total of 1200 h but were interrupted at 600 h to allow measurements to be made. The microstructural data have been collected in the grain interior and at grain...

متن کامل

The Effect of Chloride Ions Concentration on the Electrochemical Behavior of AISI 410 Stainless Steels in Simulated Concrete Pore Solution

The effect of chloride ions concentration on the electrochemical behavior of AISI 410 stainless steel in the simulated concrete pore (0.1 M NaOH + 0.1 M KOH) solution was investigated by various electrochemical methods such as Potentiodynamic polarization, Mott–Schottky analysis and electrochemical impedance spectroscopy (EIS). Potentiodynamic polarization curves revealed that increasing chlori...

متن کامل

The adhesion of hot-filament CVD diamond films on AISI type 316 austenitic stainless steel

Steel ball indentation and scratch adhesion testing of hot filament chemical vapour deposited diamond films onto AISI type 316 austenitic stainless steel substrates using two different interlayer systems, namely chromium nitride and borided steel, have been investigated. In order to compare the adhesion of these films with that of a well-known and strongly adherent system, detailed adhesion tes...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Welding and Joining

سال: 2020

ISSN: 2466-2232

DOI: 10.5781/jwj.2020.38.6.9