Sintering of Zircon Utilizing SiO<sub>2</sub>-TiO<sub>2</sub>-Al<sub>2</sub>O<sub>3</sub> Liquid Phase

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Liquid Phase Sintering of (Ti,Zr)C with WC-Co

(Ti,Zr)C powder was sintered with WC-Co following an industrial process, including an isotherm at 1410 °C. A series of interrupted sintering trials was performed with the aim of studying the sintering behavior and the microstructural evolution during both solid-state and liquid-state sintering. Reference samples, using the same elemental compositions but with the starting components TiC and ZrC...

متن کامل

An Update on the Theory of Supersolidus Liquid Phase Sintering

Prealloyed powders usually melt over a range of temperatures. This feature is useful in performing supersolidus liquid phase sintering, where liquid forms inside the particles when heated just over the solidus temperature. Densification by supersolidus liquid phase sintering is sensitive to time-temperatures. A major difficulty arises when a narrow temperature range exists between densification...

متن کامل

Processing of NiTi Foams by Transient Liquid Phase Sintering

Porous NiTi was produced by sintering pre-alloyed NiTi powders (with small Ni addition to form Ni-rich composition) with NaCl powders which are removed to create 40-60 vol.% macropores which are open to the surface, blocky in shape, and 100-400 lm in size. The microporosity present between the NiTi powders is infiltrated by an in situ created NiTi-Nb eutectic liquid which, after solidification,...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Ceramic Association, Japan

سال: 1982

ISSN: 0009-0255,1884-2127

DOI: 10.2109/jcersj1950.90.1044_420