Sintering behavior of two roughened crystals just after contact

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Harmonic lattice behavior of two-dimensional colloidal crystals.

Using positional data from videomicroscopy and applying the equipartition theorem for harmonic Hamiltonians, we determine the wave-vector-dependent normal mode spring constants of a two-dimensional colloidal model crystal and compare the measured band structure to predictions of the harmonic lattice theory. We find good agreement for both the transversal and the longitudinal modes. For q-->0, t...

متن کامل

comparative study of two silicone hydrogel contact lenses used as bandage contact lenses after photorefractive keratectomy

background: silicon hydrogel bandage contact lenses are used to enhance epithelial healing, control surface-generated pain, and prevent epithelial erosions after refractive surgery. considering the importance of faster reepithelialization in preventing complications of photorefractive keratectomy (prk) and the fact that the features and specifications of these commercially-available lenses are ...

متن کامل

Long-wavelength behavior of two-dimensional photonic crystals.

We solve analytically the multiple-scattering equations for two-dimensional photonic crystals in the long-wavelength limit. Different approximations of the electric and magnetic susceptibilities are presented from a unified pseudopotential point of view. The nature of the so-called plasmon-polariton bands is clarified. Its frequency as a function of the wire radius is discussed. The correspondi...

متن کامل

Sintering Behavior of Forsterite with Manganese Oxide as Doping Agent

Forsterite (Mg2SiO4) powder was synthesized using magnesium and talc with assistance of ball milling. Manganese doped forsterite was prepared at weight percentage of 0.05%, 0.1%, 0.2%, 0.5% and 1.0wt% by adding manganese oxide before ball milling. The undoped and manganese doped forsterite were sintered at temperature of 1000°C, 1100°C and 1200°C. The Vickers hardness, fracture toughness and Yo...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Physical Review E

سال: 2008

ISSN: 1539-3755,1550-2376

DOI: 10.1103/physreve.77.041608