RRC-Test for Weld Cracking Sensitivity of 9% Nickel Steel Electrodes

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Effect of Hydrogen Content and Welding Conditions on the Hydrogen Induced Cracking of the API X70 Steel Weld

In this study, first,diffusible hydrogen of cellulosic electrode E8010-P1 and low hydrogen electrode E8018-G was measured by mercury displacement method according to ISO3690. Then,the effect of preheating and post-heating on the sensitivity to hydrogen inducedcold cracking in welding of 18mm API5L X70 steel with these electrodes was investigated according to ISO17642-2. The results of visual in...

متن کامل

The Effect of Hydrogen Content and Welding Conditions on the Hydrogen Induced Cracking of the API X70 Steel Weld

In this study, first,diffusible hydrogen of cellulosic electrode E8010-P1 and low hydrogen electrode E8018-G was measured by mercury displacement method according to ISO3690. Then,the effect of preheating and post-heating on the sensitivity to hydrogen inducedcold cracking in welding of 18mm API5L X70 steel with these electrodes was investigated according to ISO17642-2. The results of visual in...

متن کامل

Anodized Steel Electrodes for Supercapacitors.

Steel was anodized in 10 M NaOH to enhance its surface texture and internal surface area for application as an electrode in supercapacitors. A mechanism was proposed for the anodization process. Field-emission gun scanning electron microscopy (FEGSEM) studies of anodized steel revealed that it contains a highly porous sponge like structure ideal for supercapacitor electrodes. X-ray photoelectro...

متن کامل

Transformation Plasticity in Steel Weld Metals

Professor Ulrich Dilthey’s passion for the science and technology of joining processes is amply reflected in the enormous archive of published work which will forever serve the community. It is a pleasure therefore to be able to present this small story as a tribute to someone who has been a scholar, a gentleman and a leader in this most difficult of subjects. The matter of our everyday world i...

متن کامل

Microstructural characterisation of as-deposited and reheated weld metal — High Strength Steel Weld Metals

The problems encountered with the interpretation of martensite and the various forms of bainite that are found in high strength steel weld metals have been addressed. Field emission gun scanning electron microscopy was found to overcome resolution difficulties often met with light optical microscopy and conventional scanning electron microscopy. The various microstructural constituents were cha...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Japan Welding Society

سال: 1967

ISSN: 0021-4787,1883-7204

DOI: 10.2207/qjjws1943.36.29