Rate-dependent phase transformations in nanoindented germanium
نویسندگان
چکیده
منابع مشابه
Size- and shape-dependent phase transformations in wurtzite ZnS nanostructures.
This paper describes the equilibrium morphologies of zinc sulfide nanoparticles in the wurtzite phase as a function of size, determined using ab initio Density Functional Theory (DFT) simulations and a shape-dependent thermodynamic model predicting the Gibbs free energy of a nanoparticle. We investigate the relative stabilities of a variety of nanoparticle shapes based on the wurtzite structure...
متن کاملPressure-induced morphology-dependent phase transformations of nanostructured tin dioxide
Two morphologies of nanostructured tin dioxide (SnO2) (i.e., nanobelts and nanowires) were compressed in diamond anvil cells up to 38 GPa followed by decompression. In situ Raman spectroscopy and synchrotron X-ray diffraction were employed to monitor the structural transformations. It was found that nanostructured SnO2 behaved drastically differently than bulk material in terms of transformatio...
متن کاملAdiabatic phase transformations in confinement
The phase diagram of small one-component particles has been analyzed under conditions of thermal insulation, i.e., conservation of energy. In large isolated systems the absolute stability belongs to heterogeneous states with phase separation. However, for small particles the global stability analysis shows a considerable extension of the single-phase regions into a two-phase zone of the phase d...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Applied Physics
سال: 2009
ISSN: 0021-8979,1089-7550
DOI: 10.1063/1.3151967