Sintering Properties of Mechanically Alloyed Ti-5Al-2.5Fe
In this study, Ti-5Al-2.5Fe alloy was prepared by powder metallurgy. The elemental titanium, aluminum, and iron powders were mechanically alloyed for 10 h in a vacuum atmosphere. A stainless steel jar and stainless steel balls were used for mechanical alloying. The alloyed powders were then sintered by vacuum hot pressing at 950 °C for a soaking time of 30 minutes. Pure titanium was also sinter...
متن کاملIN SITU FABRICATION OF Al 2024-Mg2Si COMPOSITE BY SPARK PLASMA SINTERING OF REACTIVE MECHANICALLY ALLOYED POWDER
In situ Al2024- Mg2Si composite was fabricated by spark plasma sintering (SPS) of reactive powder. Reactive powder was obtained from mechanical alloying (MA) of elemental powders. Clad layers of in situ composite were fabricated on Al substrates by spark plasma sintering (SPS). Structural evolution during MA process and after SPS was investigated by X-ray diffractometery (XRD). Scanning electro...
متن کاملStructural Characterization and Ordering Transformation of Mechanically Alloyed Nanocrystalline Fe-28Al Powder
The synthesis of nanocrystalline Fe3Al powder by mechanical alloying as well as the structural ordering of the synthesized Fe3Al particles during the subsequent thermal analysis were investigated. Mechanical alloying was performed up to 100 hours using a planetary ball mill apparatus with rotational speed of 300 rpm under argon atmosphere at ambient temperature. The synthesized powders were cha...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Japan Institute of Metals and Materials
سال: 1999
ISSN: 0021-4876,1880-6880
DOI: 10.2320/jinstmet1952.63.9_1161