OBJECTIVES The purpose of this study was to enhance curing light penetration through resin inlays by modifying the thicknesses of the dentin, enamel, and translucent layers. MATERIALS AND METHODS To investigate the layer dominantly affecting the power density of light curing units, resin wafers of each layer with 0.5 mm thickness were prepared and power density through resin wafers was measur...
متن کاملHardness of composite resin polymerized with different light-curing units
Introduction: The degree of polymerization depends on the type of light-curing unit. The aim of this study was to compare the hardness of composite resin cured by LED and Halogen light curing units. Methods: In this experimental study, 20 cylindrical samples of Tetric Ceram composite were prepared. Half of them were cured with Ultralume 2 LED and the other half with Astralis 7 Halogen light ...
متن کاملHardness of composite resin polymerized with different light-curing units
Introduction: The degree of polymerization depends on the type of light-curing unit. The aim of this study was to compare the hardness of composite resin cured by LED and Halogen light curing units. Methods: In this experimental study, 20 cylindrical samples of Tetric Ceram composite were prepared. Half of them were cured with Ultralume 2 LED and the other half with Astralis 7 Halogen light cur...
متن کاملColor Stability of a Microhybrid Resin Composite Polymerized with LED and QTH Light Curing Units
Introduction: Discoloration of resin composites is a common reason for replacement of these restorations. The aim of this study was to eva-luate the influence of different light curing de-vices on color stability of a microhybrid resin composite. Materials and Methods: 80 disc-shaped speci-mens (8 mm in diameter, 2-mm height) were fabricated from filtek Z250 resin composite. Specimens wer...
متن کاملLongevity of ceramic inlays and onlays luted with a solely light-curing composite resin.
OBJECTIVES To determine the longevity of heat-pressed glass ceramic inlays and onlays luted with solely light-curing composite resin. METHODS The records of patients who had received a ceramic inlay or onlay at the Heidelberg University Department of Conservative Dentistry from 1993 to 2002 were evaluated. The mean observation time and the survival probability of the ceramic inlays and onlays...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Restorative Dentistry & Endodontics
سال: 2012
ISSN: 2234-7658,2234-7666
DOI: 10.5395/rde.2012.37.3.130