Post-Weld Heat Treatment of Additively Manufactured Inconel 718 Welded to Forged Ni-Based Superalloy AD730 by Linear Friction Welding

نویسندگان

چکیده

A new post-weld heat treatment (PWHT) cycle was designed for novel dissimilar linear friction welding (LFW) of selective laser melted (SLM) Inconel 718 (IN718) to AD730 forged nickel-based superalloy. The microstructure and hardness the joints after PWHT are investigated compared with those as-linear welded samples. precipitation γ′ + γ″ is determined as main mechanism increase mechanical properties SLM IN718 alloy. These particles coarsened during at 1253 K double aging. results show that thermomechanical history can affect alloy such morphology δ phase solution (ST) from platelike in weld zone (WZ) needlelike base material (BM). It found AD730, nanometric size reprecipitated close line rapid cooling welding. presence ultrafine coarsening remaining alloy, PWHT, enhance strength hardness. developed resulted uniform across joint.

منابع مشابه

Investigation of Cutting Forces Superalloy Inconel 718

Since the cutting tools used in machining process of super alloys are subjected to high cutting forces, accordingly tools life is reduced, therefore improvement in alloys machining and reducing cutting forces to achieve longer tools life is an essential necessity. In this research, the effect of changes in feed rate on cutting forces in machining process of nickel based super alloys is investig...

متن کامل

Effect of Post-weld Heat Treatment on Joint Properties of Dissimilar Friction Stir Welded AA2024 and AA7075 Aluminum Alloys

In present study, the effect of heat treatment after friction stir welding dissimilar welds T6-7075 and T4-2024 aluminum alloys were investigated. Friction stir welding was performed at a constant rotation speed of 1140 rpm and welding speed 32 mm/min. After welding samples are taken under various heat treatment processes at different aging temperature and time period. Microstructural observati...

متن کامل

Effect of Post-weld Heat Treatment on Joint Properties of Dissimilar Friction Stir Welded AA2024 and AA7075 Aluminum Alloys

In present study, the effect of heat treatment after friction stir welding dissimilar welds T6-7075 and T4-2024 aluminum alloys were investigated. Friction stir welding was performed at a constant rotation speed of 1140 rpm and welding speed 32 mm/min. After welding samples are taken under various heat treatment processes at different aging temperature and time period. Microstructural observati...

متن کامل

Characterization of strain induced precipitation in Inconel 718 superalloy

Inconel 718 is a Ni-Cr-Fe superalloy which presents excellent mechanical properties at high temperatures, as well as good corrosion resistance and weldability. These characteristics can be optimized with an appropriate control of microstructural features such as grain size and precipitation. Precipitates of different nature can form in these alloys, i.e. γ’’ (a metastable metallic compound Ni3N...

متن کامل

Torque based weld power model for friction stir welding

For decades, models have been developed for predicting the size of the weld nugget and heat affected zones in fusion welded structures. The basis for these models is the welding heat input, which is fairly well understood for most arc welding processes. However, this traditional approach is not as straightforward for friction stir welding (FSW). To date, no definitive relationship exists to qua...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metallurgical and Materials Transactions

سال: 2021

ISSN: ['1073-5623', '1543-1940']

DOI: https://doi.org/10.1007/s11661-021-06319-0