Picosecond Laser Surface Cleaning of AM1 Superalloy
نویسندگان
چکیده
منابع مشابه
Surface acceleration during dry laser cleaning of silicon
We report on measurements of the surface acceleration for the application of dry laser cleaning. For that purpose, industrial silicon samples were irradiated by a frequency-doubled Q-switched Nd:YAG laser. The surface displacement was measured by a heterodyne interferometer and recorded by a digital storage oscilloscope. Several hundreds of shots were averaged to give smooth displacement curves...
متن کاملA Laser Assisted Dry Ice Blasting Approach for Surface Cleaning
Surface cleaning processes are needed in different life cycle phases of technical products. They are important elements in manufacturing and in maintenance during usage as well as in recycling and remanufacturing. To meet the increasing requirements in product durability and functionality, the usage of compound materials and functional coatings becomes over more important. In this regard surfac...
متن کاملOptical Near Field Effects in Surface Nanostructuring and Laser Cleaning
We present a method for directly imaging the undisturbed near field of a particle resting on a surface. A comparison with numerical computations shows good agreement with the results of our experiments. These results have important consequences for laser-assisted particle removal where field enhancement may cause local surface damage and is one of the physical key processes in this cleaning met...
متن کاملElectronically tuned picosecond Ti:sapphire laser
A widely electronically tunable picosecond Ti:sapphire laser is demonstrated without any mechanical rotation or movement for the first time. With the second harmonics of the Nd:YAG laser as a pump source, the laser produces 10 ps pulses with a maximum output power of 350 mW. The wavelength of the self-starting ultrashort laser pulses can be rapidly and arbitrarily accessed in the region from 76...
متن کاملInfrared steam laser cleaning
Steam Laser Cleaning with a pulsed infrared laser source is investigated. The infrared light is tuned to the absorption maximum of water (λ= 2.94 μm, 10 ns), whereas the substrates used are transparent (glass, silicon). Thus a thin liquid water layer condensed on top of the contaminated substrate is rapidly heated. The pressure generated during the subsequent phase explosion generates a cleanin...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Physics Procedia
سال: 2016
ISSN: 1875-3892
DOI: 10.1016/j.phpro.2016.08.020