Phase transformation strengthening of high-temperature superalloys

Decades of research has been focused on improving the high-temperature properties of nickel-based superalloys, an essential class of materials used in the hot section of jet turbine engines, allowing increased engine efficiency and reduced CO2 emissions. Here we introduce a new 'phase-transformation strengthening' mechanism that resists high-temperature creep deformation in nickel-based superal...

متن کامل

High Temperature Nanoindentation of Ni-base Superalloys

Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...

متن کامل

High Temperature Behavior of Dual Phase Steels

Dual phase steels with different martensite volume fraction and morphology were tensile tested at a temperature range of 25 to 5500C. Stress-strain curves of all steels showed serration flow at temperatures of 250 and 3500C, and smooth flow at the other temperatures. Both yield and ultimate tensile strengths increased with increasing testing temperature up to about 450<sup...

متن کامل

High Temperature Oxidation and Corrosion Properties of High Entropy Superalloys

The present work investigates the high temperature oxidation and corrosion behaviour of high entropy superalloys (HESA). A high content of various solutes in HESA leads to formation of complex oxides, however the Cr and Al activities of HESA are sufficient to promote protective chromia or alumina formation on the surface. By comparing the oxidation and corrosion resistances of a Ni-based supera...

متن کامل

Electropulsing-induced steels strengthening at high temperature

Electropulsing usually reduces the stability of metastable phases in materials. This work reports the opposite effect, where electropulsing drives the stable -phase at high temperature to be decomposed. This enables both γ-phase and σ-phase in duplex stainless steel to survive and hence to strengthen the steel at high temperature. The hardness of the quenched sample after electropulsing is 49....

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Nature Communications

سال: 2016

ISSN: 2041-1723

DOI: 10.1038/ncomms13434