New flat-punch indentation creep testing approach for characterizing the local creep properties at high temperatures

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Analysis on Pseudo-steady Indentation Creep

Theoretical analysis and finite element (FE) simulation have been carried out for a constant specific load rate (CSLR) indentation creep test. Analytical results indicate that both the representative stress and the indentation strain rate become constant after a transient period. Moreover, the FE simulation reveals that both the contours of equivalent stress and equivalent plastic strain rate u...

متن کامل

Creep Behavior of High-Strength Concrete Subjected to Elevated Temperatures

Strain is generated in concrete subjected to elevated temperatures owing to the influence of factors such as thermal expansion and design load. Such strains resulting from elevated temperatures and load can significantly influence the stability of a structure during and after a fire. In addition, the lower the water-to-binder (W-B) ratio and the smaller the quantity of aggregates in high-streng...

متن کامل

Measurement of local creep properties in stainless steel welds

A high temperature measurement system for creep deformation based on the digital image correlation (DIC) technique is described. The new system is applied to study the behaviour of a multi-pass welded joint in a high temperature tensile test and a load controlled creep test at 545°C. Spatially resolved tensile properties and time dependent creep deformation properties across a thick section typ...

متن کامل

Determination of Creep Properties for P91 Weldment Materials at 625c

The work presented in this paper is related to the determination of the creep properties for a P91 pipe weldment at 625 C, which forms part of a collaborative European project (Weldon). A Kachanov type, one damage variable, multi-axial material behaviour model was used to represent the material creep behaviour. The uniaxial material constants for the parent material and weld metal were determin...

متن کامل

Rate controlling processes in creep of close packed metals at intermediate and high temperatures

New microstructural rate controlling models for high temperature deformation are suggested which are in satisfactory agreement not only with activation parameter values but also with various metallographic observations. Non-compact slip in the HCP and FCC structures can be described by a kink pair mechanism. This process could control dislocation glide through subgrains, and therefore the creep...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials & Design

سال: 2019

ISSN: 0264-1275

DOI: 10.1016/j.matdes.2019.108090