Nanoindentation on peeled high-performance polymeric fibers reveals failure mechanisms
نویسندگان
چکیده
منابع مشابه
A FEM Multiscale Homogenization Procedure using Nanoindentation for High Performance Concrete
This paper aims to develop a numerical multiscale homogenization method for prediction of elasto-viscoplastic properties of a high performance concrete (HPC). The homogenization procedure is separated into two-levels according to the microstructure of the HPC: the mortar or matrix level and the concrete level. The elasto-viscoplastic behavior of individual microstructural phases of the matrix a...
متن کاملRapid Solidification of Polymeric Fibers
A thorough understanding of crystallization kinetics for rapid polymer solidification during the fiber spinning process is a route to maximizing fiber properties while increasing production speeds. We are using theoretical, computational, and experimental models to characterize the crystallization process at the molecular, microscopic, and macroscopic levels. Polymer dependent molecular descrip...
متن کاملFracture Failure Mechanisms of Long Single PA6 Fibers
The present study investigates the failure mechanisms of industrial fiber materials, using a custom designed fiber cutting performance test bench. The fracture morphologies of single PA6 fibers are examined by scanning electron microscopy. The analysis reveals that fiber cutting can be distinguished according to four distinct stages of fiber failure represented by shearing, cutting, brittle fra...
متن کاملCharacterization of Viscoelastic Properties of Polymeric Materials through Nanoindentation
Nanoindentation is used to determine the dynamic viscoelastic properties of six polymer materials. It is shown that varying the harmonic frequency of the nanoindentation does not have any significant effect on the measured storage and loss moduli of the polymers. Agreement is found between these results and data from DMA testing of the same materials. Varying the harmonic amplitude of the nanoi...
متن کاملImprovement of Strength Parameters of Sand Reinforced with Polymeric Fibers
Triaxial consolidated drained, unconfined compression, and CBR tests have been conducted in order to study the stress-strain, strength, and volume change characteristics of fine sand specimens reinforced by polymeric fibers made from carpet wastes. The variables are aspect ratio (length/width) and weight percentage of the fibers. The results indicate that the peak strength and total volume chan...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: MRS Bulletin
سال: 2020
ISSN: 0883-7694,1938-1425
DOI: 10.1557/mrs.2020.257