Nanoindentation and wear behavior of thermally stable biocompatible polysulfone–alumina nanocomposites

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Wear Behavior of Composites and Nanocomposites: A New Approach

The expulsion of material from either of two strong surfaces in relative movement is termed as wear. Wear can also be defined as surface damage, because of material relocation with no net change in weight or volume. It happens as a natural result and for the most part through surface interactions at severities. It is a system response and is not a material property. Interface wear is firmly com...

متن کامل

Thermally Stable Poly(amide-imide)/Nanocomposites Reinforced Silicate Nanoparticles Containing Bicyclo Segment and Dibenzalacetone Moiety: Synthesis and Characterization

Two new samples of poly(amide-imide)/nanocomposites containing bicyclo segment and dibenzalaceton moiety in the main chain were synthesized by a solution intercalation technique. Poly(amide-imide) (PAI) 8 as a source of polymer matrix was synthesized by the direct polycondensation reaction of N,N´-bis(4-carboxyphenyl)bicyclo[2,2,2]oct-7-ene-2,3,5,6-tetracarboxylic diimide 3 with 2,6-bis(4-amino...

متن کامل

Thermally Stable Poly(amide-imide)/Nanocomposites Reinforced Silicate Nanoparticles Containing Bicyclo Segment and Dibenzalacetone Moiety: Synthesis and Characterization

Two new samples of poly(amide-imide)/nanocomposites containing bicyclo segment and dibenzalaceton moiety in the main chain were synthesized by a solution intercalation technique. Poly(amide-imide) (PAI) 8 as a source of polymer matrix was synthesized by the direct polycondensation reaction of N,N´-bis(4-carboxyphenyl)bicyclo[2,2,2]oct-7-ene-2,3,5,6-tetracarboxylic diimide 3 with 2,6-bis(4-amino...

متن کامل

thermally stable poly(amide-imide)/nanocomposites reinforced silicate nanoparticles containing bicyclo segment and dibenzalacetone moiety: synthesis and characterization

two new samples of poly(amide-imide)/nanocomposites containing bicyclo segment and dibenzalaceton moiety in the main chain were synthesized by a solution intercalation technique. poly(amide-imide) (pai) 8 as a source of polymer matrix was synthesized by the direct polycondensation reaction of n,n´-bis(4-carboxyphenyl)bicyclo[2,2,2]oct-7-ene-2,3,5,6-tetracarboxylic diimide 3 with 2,6-bis(4-amino...

متن کامل

Preparation and Properties of Thermally Stable Polyureas Containing Ether and Ketone Units

The main objective of this search was to prepare novel soluble polyureas with improved thermal stability. Accordingly, a new types of polyureas was prepared through the polycondensation reaction of a prepared diamine containing ether, keto, and naphthyl groups with 4,4’-diphenylmethan diisocyanate (MDI), toluene-2,4-diisocyanate (TDI), and isophorone diisocyanate (IPDI) in N-methyl-2-pyrrol...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: RSC Advances

سال: 2016

ISSN: 2046-2069

DOI: 10.1039/c6ra20838j