Growth and Characterization of Thin MoS2 Films by Low- Temperature Chemical Bath Deposition Method

Transition metal dichalcogenide (TMDC) materials are very important inelectronic and optical integrated circuits and their growth is of great importance in thisfield. In this paper we present growth and fabrication of MoS2 (Molibdan DiSulfide)thin films by chemical bath method (CBD). The CBD method of growth makes itpossible to simply grow large area scale of the thin la...

متن کامل

Low Temperature Atomic Layer Deposition of Tin Oxide

Atomic layer deposition (ALD) of tin oxide (SnOx) films was achieved using a newly synthesized tin precursor and hydrogen peroxide. We obtained highly pure, conductive SnOx films at temperatures as low as 50 C, which was possible because of high chemical reactivity between the new Sn precursor and hydrogen peroxide. The growth per cycle is around 0.18 nm/cycle in the ALDwindow up to 150 C, and ...

متن کامل

Low-temperature formation of silicon nitride gate dielectrics by atomic-layer deposition

Thin ~equivalent oxide thickness Teq of 2.4 nm! silicon nitride layers were deposited on Si substrates by an atomic-layer-deposition ~ALD! technique at low temperatures ~,550 °C!. The interface state density at the ALD silicon nitride/Si-substrate interface was almost the same as that of the gate SiO2. No hysteresis was observed in the gate capacitance–gate voltage characteristics. The gate lea...

متن کامل

Low temperature silicon dioxide by thermal atomic layer deposition: Investigation of material properties

Investigation of material properties D. Hiller, R. Zierold, J. Bachmann, M. Alexe, Y. Yang, J. W. Gerlach, A. Stesmans, M. Jivanescu, U. Müller, J. Vogt, H. Hilmer, P. Löper, M. Künle, F. Munnik, K. Nielsch, and M. Zacharias Faculty of Engineering, IMTEK, Albert-Ludwigs-University Freiburg, Georges-Köhler-Allee 103, 79110 Freiburg, Germany Max Planck Institute of Microstructure Physics, Weinber...

متن کامل

Low-temperature atomic layer epitaxy of AlN ultrathin films by layer-by-layer, in-situ atomic layer annealing

Low-temperature epitaxial growth of AlN ultrathin films was realized by atomic layer deposition (ALD) together with the layer-by-layer, in-situ atomic layer annealing (ALA), instead of a high growth temperature which is needed in conventional epitaxial growth techniques. By applying the ALA with the Ar plasma treatment in each ALD cycle, the AlN thin film was converted dramatically from the amo...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Nanoscale

سال: 2020

ISSN: 2040-3364,2040-3372

DOI: 10.1039/d0nr03863f