Modified Shrinking Core Model for Atomic Layer Deposition of TiO2on Porous Alumina with Ultrahigh Aspect Ratio

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Mechanisms of atomic layer deposition on substrates with ultrahigh aspect ratios.

Atomic layer deposition (ALD) appears to be uniquely suited for coating substrates with ultrahigh aspect ratios (> or similar 10(3)), including nanoporous solids. Here, we study the ALD of Cu and Cu3N on the inner surfaces of low-density nanoporous silica aerogel monoliths. Results show that Cu depth profiles in nanoporous monoliths are limited not only by Knudsen diffusion of heavier precursor...

متن کامل

Atomic Layer Deposition for Coating of High Aspect Ratio TiO2 Nanotube Layers

We present an optimized approach for the deposition of Al2O3 (as a model secondary material) coating into high aspect ratio (≈180) anodic TiO2 nanotube layers using the atomic layer deposition (ALD) process. In order to study the influence of the diffusion of the Al2O3 precursors on the resulting coating thickness, ALD processes with different exposure times (i.e., 0.5, 2, 5, and 10 s) of the t...

متن کامل

Porous Alumina Protective Coatings on Palladium Nanoparticles by Self-Poisoned Atomic Layer Deposition

Atomic layer deposition (ALD) of Al2O3 using trimethylaluminum (TMA) and water on Pd nanoparticles (NPs) was studied by combining in situ quartz crystal microbalance (QCM) measurements, in situ quadrupole mass spectrometry (QMS), and transmission electron microscopy (TEM) with density functional theory (DFT) calculations. TEM images of the ALD Al2O3 overcoated Pd showed conformal Al2O3 films on...

متن کامل

Atomic layer deposition in porous structures: 3D photonic crystals

This paper reports recent results from studies of atomic layer deposition for the infiltration of three-dimensional photonic crystals. Infiltration of ZnS:Mn and TiO2 are reported for SiO2-based opal templates. It has been demonstrated that high filling fractions can be achieved and that the infiltrated material can be of high crystalline quality as assessed by photoluminescence measurements. T...

متن کامل

SERS Taper-Fiber Nanoprobe Modified by Gold Nanoparticles Wrapped with Ultrathin Alumina Film by Atomic Layer Deposition

A taper-fiber SERS nanoprobe modified by gold nanoparticles (Au-NPs) with ultrathin alumina layers was fabricated and its ability to perform remote Raman detection was demonstrated. The taper-fiber nanoprobe (TFNP) with a nanoscale tip size under 80 nm was made by heated pulling combined with the chemical etching method. The Au-NPs were deposited on the TFNP surface with the electrostatic self-...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Bulletin of the Korean Chemical Society

سال: 2013

ISSN: 0253-2964

DOI: 10.5012/bkcs.2013.34.2.519