Microstructure, Mechanical Properties and Thermal Stability of Ni-Based Single Crystal Superalloys with Low Specific Weight

نویسندگان

چکیده

Ni-based single crystal (SX) superalloy with low specific weight is vital for developing aero engines a high strength-to-weight ratio. Based on an alloy system 3 wt.% Re but without W, namely Ni-Co-Cr-Mo-Ta-Re-Al-Ti, below 8.4 g/cm3 has been achieved. To reveal the relationship among composition, mechanical properties, and thermal stability of SX superalloys, SXs desirable microstructures are fabricated. Tensile tests revealed that alloys have comparable strength to commercial second-generation CMSX-4 (3 6 W) Rene? N5 5 above 800 °C. Moreover, elongation fracture (EF) 850 °C (>20%) better than those two superalloys. During exposure at 1050 up 500 h, topological close-packed (TCP) phase does not appear, indicating excellent stability. Decreasing Al concentration increases resistance ?? rafting replacing 1 Ti Ta beneficial shape size during exposure. The current work might provide scientific insights superalloys weight.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Evaluating the Effect of Ta/W Ratio on Microstructure and Stress Rupture Properties of Ni-Based Single Crystal Superalloy PWA1483

In this study, the effect of Ta/W ratio on the microstructure and stress rupture properties of Ni-based single crystal (SX) superalloy PWA1483 was investigated. For this purpose, single crystal (SX) superalloys with different Ta/W ratios (0.75, 1.0, 1.32 and 1.5 in wt.%) were fabricated. The alloys were directionally solidified by Bridgman method under the same solidification condition at withd...

متن کامل

determination of some physical and mechanical properties red bean

چکیده: در این تحقیق، برخی خواص فیزیکی و مکانیکی لوبیا قرمز به-صورت تابعی از محتوی رطوبت بررسی شد. نتایج نشان داد که رطوبت بر خواص فیزیکی لوبیا قرمز شامل طول، عرض، ضخامت، قطر متوسط هندسی، قطر متوسط حسابی، سطح تصویر شده، حجم، چگالی توده، تخلخل، وزن هزار دانه و زاویه ی استقرار استاتیکی در سطح احتمال 1 درصد اثر معنی داری دارد. به طوری که با افزایش رطوبت از 54/7 به 12 درصد بر پایه خشک طول، عرض، ضخام...

15 صفحه اول

MODELLING THE MATERIAL PROPERTIES AND BEHAVIOUR OF Ni-BASED SUPERALLOYS

At the last two Superalloy meetings at Seven Springs, work on the development of thermodynamic modelling tools for application to multi-component Ni-based superalloys has been presented. Such modelling has become quite widespread, providing significant benefit. However, its applicability often falls short from directly providing the information that is actually required and, by itself, cannot b...

متن کامل

Influence of Cu and Ni on the Microstructure and Mechanical Properties of an HSLA Steel

In this research the role of alloying elements on the microstructure and mechanical properties of an as cast and hot rolled high strength low alloy (HSLA) steel was studied. Different compositions with different amount of copper in the presence of nickel, hot rolled and quenched in oil. Tensile test, hardness test, scanning electron microscope (SEM) and optical microscope (OM) were used to eval...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Crystals

سال: 2023

ISSN: ['2073-4352']

DOI: https://doi.org/10.3390/cryst13040610