Mechanical Properties of Inconel 718 Nickel-Based Superalloy around Solidus Temperature
نویسندگان
چکیده
منابع مشابه
Effect of Thermomechanical Working on the Microstructure and Mechanical Properties of Hot Pressed Superalloy Inconel 718
Experimental results on hot deformation and dynamic structural processes of nickel based alloy Inconel 718 are reviewed. The focus is the analysis of dynamic precipitation processes which operate during hot deformation of these materials at elevated temperatures. Hot compression tests were performed on the solution treated precipitation hardenable nickel based superalloy Inconel 718 at 720-1150...
متن کاملInvestigation of Cutting Forces Superalloy Inconel 718
Since the cutting tools used in machining process of super alloys are subjected to high cutting forces, accordingly tools life is reduced, therefore improvement in alloys machining and reducing cutting forces to achieve longer tools life is an essential necessity. In this research, the effect of changes in feed rate on cutting forces in machining process of nickel based super alloys is investig...
متن کاملCharacterization of strain induced precipitation in Inconel 718 superalloy
Inconel 718 is a Ni-Cr-Fe superalloy which presents excellent mechanical properties at high temperatures, as well as good corrosion resistance and weldability. These characteristics can be optimized with an appropriate control of microstructural features such as grain size and precipitation. Precipitates of different nature can form in these alloys, i.e. γ’’ (a metastable metallic compound Ni3N...
متن کاملSelective Growth of Low Stored Energy Grains During δ Sub-solvus Annealing in the Inconel 718 Nickel-Based Superalloy
The microstructure stability during d sub-solvus annealing in Inconel 718 was investigated, focusing on the conditions that may lead to the development of very large grains (about 100 lm) in a recrystallized fine grained matrix (4 to 5 lm) despite the presence of second-phase particles. Microstructure evolution was analyzed by EBSD (grain size, intragranular misorientation) and SEM (d phase par...
متن کاملHigh temperature fatigue crack propagation behaviour of Inconel 718
The overall objective of this work has been to develop and evaluate tools for designing against fatigue in gas turbine applications, with special focus on the nickelbased superalloy Inconel 718. The fatigue crack propagation behaviour under high temperature hold times has been studied. Firstly, the main fatigue crack propagation phenomena have been investigated with the aim of setting up a basi...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Japan Institute of Metals
سال: 2012
ISSN: 1880-6880,0021-4876