Low Temperature Sintering and Electrical Properties of Bi-based ZnO Chip Varistor

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Influence of Adding SiC on Microstructure and Electrical Properties of ZnO-based Nanocomposite Varistor

In this research the influence of adding SiC on microstructure and electrical properties of ZnO-based Nanocomposite varistors were investigated. SiC was added with amounts of 10-0 mass% to ZnO-based varistor composition. It is found that SiC allows reaching to high threshold voltage with formation of fine-graine...

متن کامل

influence of adding sic on microstructure and electrical properties of zno-based nanocomposite varistor

in this research the influence of adding sic on microstructure and electrical properties of zno-based nanocomposite varistors were investigated. sic was added with amounts of 10-0 mass% to zno-based varistor composition. it is found that sic allows reaching to high threshold voltage with formation of fine-grained zno.another important effect of adding sic is formation zn2sio4 (willemite) on the ...

متن کامل

Optimization of Bi2O3, TiO2, and Sb2O3 Doped ZnO-Based Low-Voltage Varistor Ceramic to Maximize Nonlinear Electrical Properties

In ZnO-based low voltage varistor, the two essential features of microstructure determining its nonlinear response are the formation Bi-enriched active grain boundaries as well as a controlled ZnO grain size by secondary spinel-type phases. Besides, the microstructure and phase composition are strongly affected by the dopant concentration during sintering process. In this study, the optimal dop...

متن کامل

LOW-TEMPERATURE SINTERING OF HIGH VOLTAGE GRADIENT ZnO-BASED THICK FILM VARISTORS

High voltage gradient ZnO-based thick film varistors were fabricated by low-temperature sintering. The effect of sintering temperature on electrical properties of thick film varistors was investigated. The voltage gradient of thick film varistors increased significantly to 3159.4 V/mm after sintering at 725°C for 30 min. The small average grain size with good grain boundaries was the origin for...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Korean Institute of Electrical and Electronic Material Engineers

سال: 2011

ISSN: 1226-7945

DOI: 10.4313/jkem.2011.24.11.876