Leaching of Zinc Oxide in Acidic Solution

Leaching mechanism of zinc oxide is important not only to understand zinc smelting process but also to develop of new zinc recycling process. Recycling of zinc is mainly done by treatment of electric arc furnace dust (EAF dust). In Japan pyro metallurgical process is enhanced for EAF dust treatment, however only zinc oxide can be recovered by pyro metallurgical process. Hydro metallurgical proc...

متن کامل

Solution-grown zinc oxide nanowires.

We review two strategies for growing ZnO nanowires from zinc salts in aqueous and organic solvents. Wire arrays with diameters in the nanoscale regime can be grown in an aqueous solution of zinc nitrate and hexamethylenetetramine. With the addition of poly(ethylenimine), the lengths of the wires have been increased to 25 mum with aspect ratios over 125. Additionally, these arrays were made vert...

متن کامل

Leaching of Lead and Zinc from a Low-Grade Oxide Ore in Citric Acid Media

Leaching of a low-grade lead and zinc oxide ore was studied by an organic reagent, citric acid. The quadratic mathematical models were developed for the relationship among the influential parameters and lead and zinc recoveries. Leaching rate was strongly affected by the interactive effects of factors. It was also found that the quadratic effects of stirring speed and linear<e...

متن کامل

Microwave and Ultrasound Augmented Leaching of Complicated Zinc Oxide Ores in Ammonia and Ammonium Citrate Solutions

Recovery of zinc from low grade zinc oxide ore is attempted with ammonia and ammonium citrate solutions augmented by microwave roasting and ultrasound radiation. The influence of the ammonia-ammonium ratio, roasting temperature, ultrasound power, and leaching time were assessed on the recovery of zinc. A maximum zinc recovery of 88.57% could be achieved at a roasting temperature of 673 K, leach...

متن کامل

Preparation of Cobalt Oxide/Zinc Oxide Nanocomposite

Cobalt Oxide/ Zinc Oxide nanocomposite was synthesized by dropwise addition ofCo(NO)3.6H2O and Zn(NO3)2.4H2O solutions to KOH solution at different temperatures followed bycalcination at 300ºC for 4 h. The morphology and structure of nanoparticles and the influence oftemperature on particle size were studied using scanning electron microscopy (SEM) and X-RayDiffraction (XRD). Minimum particle s...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: MATERIALS TRANSACTIONS

سال: 2003

ISSN: 1345-9678,1347-5320

DOI: 10.2320/matertrans.44.2489