Investigations into stress corrosion cracking behaviour of AZ91D magnesium alloy in physiological environment

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of heat treatment on corrosion and electrochemical behaviour of AZ91D magnesium alloy

An AZ91D ingot in the as-cast condition was homogenized by solution treatment and then aged for various periods of time. The microstructures produced were studied in detail and the b phase volume fraction was measured quantitatively. The Corrosion resistance of all the different microstructures was studied in 3.5% NaCl solution through weight loss measurement in constant immersion conditions an...

متن کامل

Studies on the in ̄uence of chloride ion and pH on the corrosion and electrochemical behaviour of AZ91D magnesium alloy

The in ̄uence of chloride ion concentration and pH on the corrosion and electrochemical behaviour of die-cast and ingot-cast AZ91D alloy have been studied with a focus on the stability of microconstituents in these environments. The experimental techniques used include immersion studies, potentiodynamic polarization, X-ray di€raction and optical and scanning electron microscopy. The corrosion ra...

متن کامل

Hot cracking in tungsten inert gas welding of magnesium alloy AZ91D

Plates of 3–5 mm in thickness were extracted from an AZ91D ingot and then butt joints of the plates were produced using tungsten inert gas (TIG) welding method. The TIG arc was also used to deposit welding beads on some of the thin plates. No cracking was found in the butt joints. However, hot cracking was always observed to propagate from the heat affected zone (HAZ) under the welding bead int...

متن کامل

Influence of Zeolite Coating on the Corrosion Resistance of AZ91D Magnesium Alloy

The protective performance of zeolite coating on AZ91D magnesium alloy was evaluated using potentiodynamic polarisation and electrochemical impedance spectroscopy (EIS) in 0.1 M sodium chloride solution (NaCl). Electrical equivalent circuit (EEC) was developed based upon hypothetical corrosion mechanisms and simulated to correspond to the experimental data. The morphology and the chemical natur...

متن کامل

Influence of Sulfate-Reducing Bacteria on the Corrosion Residual Strength of an AZ91D Magnesium Alloy

In this paper, the corrosion residual strength of the AZ91D magnesium alloy in the presence of sulfate-reducing bacteria is studied. In the experiments, the chemical composition of corrosion film was analyzed by a scanning electron microscope with energy dispersive X-ray spectroscopy. In addition, a series of instruments, such as scanning electronic microscope, pH-meter and an AG-10TA materials...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Procedia Engineering

سال: 2011

ISSN: 1877-7058

DOI: 10.1016/j.proeng.2011.04.087