Interfacial microstructure and strength of magnetic pulse welded A5052 aluminum alloy/SPCC steel lap joint

نویسندگان

چکیده

A5052 aluminum alloy and SPCC steel plates were welded using magnetic pulse welding, interfacial microstructure strength of the lap joint examined. The used for a flyer plate parent plate, respectively. Charging energy stored in capacitor gap between changed. Microstructure was examined by an optical microscope, scanning electron microscope transmission microscope. Tensile-shear test evaluating joint. welding achieved at charging above 6.0 kJ 1.0 mm. range which strong is accomplished different each increased with decreasing gap. not fractured interface tensile-shear whereas fracture occurred part base metal. exhibited characteristic wavy morphology. An intermediate layer produced along interface. Scanning observation revealed that composed fine Al-Mg grains dispersed dendritic Al-Fe intermetallic compound particles.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Microstructure Evolution and Shaping of Friction Stir Lap Welded Dissimilar Magnesium Alloy Joint

Friction stir lap welding (FSLW) experiment has been conducted on 3mm thick AZ80 extruded sheet and 2.3mm thick AZ31B rolled sheet. The influence of the shape of the taper thread mixing head on microstructure has been discussed. Pores forming, hooked defects, interface migration, tissue distribution have been analyzed. The organization of both sides of nugget zone (NZ) is arranged diagonally ab...

متن کامل

Microstructure and Mechanical Properties of the Friction Welded Joint between X53CrMnNiN219 and X45CrSi93 Stainless Steel

Dissimilar metals friction welding of austenitic–martensitic stainless steels is commonly used in order to manufacture engine valves in the automobile industry. In this study, X53CrMnNiN219 (austenitic stainless steel) and X45CrSi93 (martensitic stainless steel) valve steel rods were welded by friction welding process. The welded joint was then heat treated at 760 0C for 60 min. Mechanical prop...

متن کامل

microstructure and mechanical properties of the friction welded joint between x53crmnnin219 and x45crsi93 stainless steel

dissimilar metals friction welding of austenitic–martensitic stainless steels is commonly used in order to manufacture engine valves in the automobile industry. in this study, x53crmnnin219 (austenitic stainless steel) and x45crsi93 (martensitic stainless steel) valve steel rods were welded by friction welding process. the welded joint was then heat treated at 760 0c for 60 min. mechanical prop...

متن کامل

Investigation of Standoff Distance Effect on Corrosion Behavior of Explosively Welded Joint between Two Aluminum Plates and Steel

In the present research, the effect of standoff distance on corrosion properties of the joint of three aluminum–steel explosive layers has been studied. For this purpose, the samples were welded with various standoff distance under constant explosive load. Optical Microscopy and Scanning Electron Microscopy were used to measure the quality of the joint and type of interface. Furthermore, point ...

متن کامل

Real-time monitoring of laser welding of galvanized high strength steel in lap joint configuration

Two different cases regarding the zinc coating at the lap joint faying surface are selected for studying the influence of zinc vapor on the keyhole dynamics of the weld pool and the final welding quality. One case has the zinc coating fully removed at the faying surface; while the other case retains the zinc coating on the faying surface. It is found that removal of the zinc coating at the fayi...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Japan Institute of Light Metals

سال: 2023

ISSN: ['0451-5994', '1880-8018']

DOI: https://doi.org/10.2464/jilm.73.99