Identification and Quantification of Microplastics in Effluents of Wastewater Treatment Plant by Differential Scanning Calorimetry (DSC)
نویسندگان
چکیده
In this research, the presence of microplastics was detected through a differential scanning calorimetry (DSC) analysis three wastewater treatment plants. One these plants applied only preliminary stage while others up to secondary evaluate their effectiveness. The results showed polyethylene (PE), polystyrene (PS), polypropylene (PP) and terephthalate (PET), which were classified as fragments, fibers or granules. During evaluation plants, it determined that did not remove more than 58% microplastics, applying with activated sludge achieved microplastic removal effectiveness between 90% 96.9%.
منابع مشابه
Surveying the effects of silver nanoparticle on thermal properties of some calyx [4]arene compounds by Differential Scanning Calorimetry (DSC)
One of the best and the most active ways for surveying thermal behaviour of materials is using differential scanning calorimetry. In this paper, the authors have studied thermal behaviour for Schiff base ligand and their synthesized Cobalt, Nickel complexes. In this method, the sample is opposed to a controlled temperature change and its physical properties. Here we studied melting point and Tg...
متن کاملSurveying the effects of silver nanoparticle on thermal properties of some calyx [4]arene compounds by Differential Scanning Calorimetry (DSC)
One of the best and the most active ways for surveying thermal behaviour of materials is using differential scanning calorimetry. In this paper, the authors have studied thermal behaviour for Schiff base ligand and their synthesized Cobalt, Nickel complexes. In this method, the sample is opposed to a controlled temperature change and its physical properties. Here we studied melting point and Tg...
متن کاملPractical Food Applications of Differential Scanning Calorimetry (DSC)
This note describes a number of important food applications utilising the PerkinElmer DSC demonstrating the versatility of the technique as a tool in the food industry.
متن کاملIdentification and quantification of estrogen receptor agonists in wastewater effluents.
Total concentrations of several known xenobiotic estrogen receptor (ER) agonists and natural and synthetic estrogen were measured in water by use of a combination of instrumental and bioanalytical approaches. Samples from 3 municipal wastewater treatment plants (WWTPs) in south central Michigan (upstream and effluent); 4 point source locations on the Trenton Channel of the Detroit River, MI; an...
متن کاملDetermination of the activation energy of crystallization based up on Ozawa and Kissinger formalisms and thermal stability of V2O5-NiO- TeO2 glasses by differential scanning calorimetry (DSC)
In the present research work, (60-x)V2O5-xNiO-40TeO2 amorphous bulk compositions with different molar percentages of 0≤x≤20 mol%, were prepared by well-known rapid melt-quenching method. Differential scanning calorimetry (DSC) at different heating rates (φ) was used to thermal analyze and to obtain more insight in to the thermal stability, glass forming tendency and so calorimetric characteris...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Sustainability
سال: 2022
ISSN: ['2071-1050']
DOI: https://doi.org/10.3390/su14094920