Hydrogen and Deuterium Incorporation in ZnO Films Grown by Atomic Layer Deposition

نویسندگان

چکیده

Zinc oxide (ZnO) thin films were grown by atomic layer deposition using diethylzinc (DEZ) and water. In addition to depositions with normal water, heavy water (2H2O) was used in order study the reaction mechanisms hydrogen incorporation at different temperatures from 30 200 ?C. The total concentration found increase as temperature decreased. When decreased close room temperature, main source of impurity changed 1H 2H. A sufficiently long purging time isotope incorporated film back 1H. multiple short pulse scheme transient steric hindrance. addition, effect storage samples ambient conditions studied. During storage, deuterium while increased an equal amount, indicating that there exchange H2 and/or H2O.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effects of doping and annealing on properties of ZnO films grown by atomic layer deposition

Undoped and Al-doped ZnO films were synthesized by atomic layer deposition at 150°C and then annealed at 350°C in different atmospheres. Effects of doping and annealing on the film growth mode and properties were investigated. The undoped film has strong UV emission and weak Zn interstitial emission. Annealing introduces O vacancies, decreases Zn interstitials, and results in weakening and blue...

متن کامل

Enhanced visible photoluminescence from ultrathin ZnO films grown on Si-nanowires by atomic layer deposition.

Bright room temperature visible emission is obtained in heterostructures consisting of approximately 3.5 nm thick ZnO ultrathin films grown on Si-nanowires produced by means of self-masking dry etching in hydrogen-containing plasma. The ZnO films were deposited on Si-nanowires by using atomic layer deposition (ALD) under an ambient temperature of 25 degrees C. The orders of magnitude enhancemen...

متن کامل

(Sn,Al)Ox Films Grown by Atomic Layer Deposition

Tin oxide (SnO2) is a transparent semiconductor with a wide band gap and electrical resistivity as low as 2 10 4 Ω 3 cm and high infrared reflectivity, over 90%. 4 These properties are achieved using n-type doping by substituting fluorine for about 1% of the oxygen. The low electrical resistance and optical transparency in SnO2 are widely used in applications such as solar cells, displays, touc...

متن کامل

Evolution of microstructure and related optical properties of ZnO grown by atomic layer deposition

A study of transmittance and photoluminescence spectra on the growth of oxygen-rich ultra-thin ZnO films prepared by atomic layer deposition is reported. The structural transition from an amorphous to a polycrystalline state is observed upon increasing the thickness. The unusual behavior of the energy gap with thickness reflected by optical properties is attributed to the improvement of the cry...

متن کامل

Electrical transport and Al doping efficiency in nanoscale ZnO films prepared by atomic layer deposition

• A submitted manuscript is the author's version of the article upon submission and before peer-review. There can be important differences between the submitted version and the official published version of record. People interested in the research are advised to contact the author for the final version of the publication, or visit the DOI to the publisher's website. • The final author version ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Coatings

سال: 2021

ISSN: ['2079-6412']

DOI: https://doi.org/10.3390/coatings11050542