Hybrid inorganic–organic superlattice structures with atomic layer deposition/molecular layer deposition

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Atomic Layer Deposition of TiO

Additional resources and features associated with this article are available within the HTML version: • Supporting Information • Links to the 4 articles that cite this article, as of the time of this article download • Access to high resolution figures • Links to articles and content related to this article • Copyright permission to reproduce figures and/or text from this article High surface a...

متن کامل

Impact of Atomic Layer Deposition to Nanophotonic Structures and Devices

*Correspondence: Muhammad Rizwan Saleem, Center for Energy Systems (CES), USAID Center for Advance Studies, National University of Sciences and Technology (NUST), Sector H-12, Islamabad 44000, Pakistan e-mail: [email protected]; [email protected] We review the significance of optical thin films by Atomic Layer Deposition (ALD) method to fabricate nanophotonic devices and structures. A...

متن کامل

Atomic layer deposition in porous structures: 3D photonic crystals

This paper reports recent results from studies of atomic layer deposition for the infiltration of three-dimensional photonic crystals. Infiltration of ZnS:Mn and TiO2 are reported for SiO2-based opal templates. It has been demonstrated that high filling fractions can be achieved and that the infiltrated material can be of high crystalline quality as assessed by photoluminescence measurements. T...

متن کامل

Atomic layer deposition (ALD): from precursors to thin film structures

The principles of the atomic layer deposition (ALD) method are presented emphasizing the importance of precursor and surface chemistry. With a proper adjustment of the experimental conditions, i.e. temperatures and pulsing times, the growth proceeds via saturative steps. Selected recent ALD processes developed for films used in microelectronics are described as examples. These include depositio...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films

سال: 2014

ISSN: 0734-2101,1520-8559

DOI: 10.1116/1.4831751