History and Remained Subject on Standardized Corrosion Test Methods. IV: Techniques for Evaluating Pitting Corrosion and Crevice Corrosion.

نویسندگان

چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Roughness, Residual Stresses and Pitting Corrosion Effect on Shot

Original scientific paper The paper deals with the effect of roughness, residual stresses and pitting corrosion on different shot peened (SP) ENAW 7075 aluminium alloy in different states. Suitable residual stress profile increases the applicability and life cycle of mechanical parts, treated by shot peening. Pitting corrosion has a major influence on aging of structural elements made of high s...

متن کامل

Corrosion pitting and environmentally assisted small crack growth.

In many applications, corrosion pits act as precursors to cracking, but qualitative and quantitative prediction of damage evolution has been hampered by lack of insights into the process by which a crack develops from a pit. An overview is given of recent breakthroughs in characterization and understanding of the pit-to-crack transition using advanced three-dimensional imaging techniques such a...

متن کامل

Pitting Corrosion Behaviour of New Corrosion-Resistant Reinforcement Bars in Chloride-Containing Concrete Pore Solution

In this study, the pitting behaviour of a new corrosion-resistant alloy steel (CR) is compared to that of low-carbon steel (LC) in a simulated concrete pore solution with a chloride concentration of 5 mol/L. The electrochemical behaviour of the bars was characterised using linear polarisation resistance (LPR) and electrochemical impedance spectroscopy (EIS). The pitting profiles were detected b...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Society of Materials Science, Japan

سال: 1996

ISSN: 1880-7488,0514-5163

DOI: 10.2472/jsms.45.1248