High-reliability repair of single-crystal Ni-base superalloy by selective electron beam melting

نویسندگان

چکیده

Here, we report the utilisation of a powder-bed-fusion additive manufacturing to achieve CMSX-4 single-crystal repair with René N5 powders. The is characterised by fine columnar dendritic substructure, limited in-grain misorientation over tens millimetres in height, and strong deposit-to-substrate bonding. brighter contrast region 300 400 μm thick, formed cellular solidification front, sits above melted back horizontal low-angle boundary (4° misorientation) in-between. Its higher hardness 450 HV attributed cuboidal primary γ′ 135 ± 7 nm. Their presence combined effect high cooling rate local compositional difference. Scheil-Gulliver predicted solute partitioning Ta Hf inter-dendritic agrees well MC carbides appearing at boundaries. Computational-fluid-dynamics (CFD) simulations, minimum undercooling criterion, helps determine vertical distance between melt-pool bottom oriented-to-misoriented transition borderline, providing convenient guideline assess likelihood, sense that this needs be larger than hatch depth. CFD-calculated velocities thermal gradients agree columnar-to-equiaxed curve experimental observation.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Open-Cellular Co-Base and Ni-Base Superalloys Fabricated by Electron Beam Melting

Reticulated mesh samples of Co-29Cr-6Mo alloy and Ni-21Cr-9Mo-4Nb alloy (625) and stochastic foam samples of Co-29Cr-6Mo alloy fabricated by electron beam melting were characterized by optical metallography, and the dynamic stiffness (Young's modulus) was measured by resonant frequency analysis. The relative stiffness (E/Es) versus relative density (ρ/ρs) plotted on a log-log basis resulted in ...

متن کامل

Fretting on the cubic face of a single-crystal Ni-base superalloy at room temperature

Fretting experiments were conducted on the (10 0) crystal (cubic) face of a single crystal Ni-base superalloy in two directions, /10 0S and /110S, to study the effect of crystallographic orientation on the fretting response in both partial slip and gross slip regimes. The study involved point contacts using a tungsten carbide (WC) ball with radius 10 mm tested at room temperature. Ball indentat...

متن کامل

Evaluating the Effect of Ta/W Ratio on Microstructure and Stress Rupture Properties of Ni-Based Single Crystal Superalloy PWA1483

In this study, the effect of Ta/W ratio on the microstructure and stress rupture properties of Ni-based single crystal (SX) superalloy PWA1483 was investigated. For this purpose, single crystal (SX) superalloys with different Ta/W ratios (0.75, 1.0, 1.32 and 1.5 in wt.%) were fabricated. The alloys were directionally solidified by Bridgman method under the same solidification condition at withd...

متن کامل

Creep Crack Growth Simulation of Ni-base Superalloy

The purpose of this study is to develop a numerical approach to simulate the creep cracking of a Ni-base superalloy. The approach is based in continuum damage mechanics (CDM) and uses the classic Kachanov-Rabotnov constitutive equations for creep deformation and damage evolution. Creep damage takes the form of defects such as microcracks, cavities, voids, etc. A numerical crack growth algorithm...

متن کامل

Joining of nickel-base superalloy single crystals

Introduction ................................................................................................................................1 Overview of Weldability of Nickel-Base Superalloys..................................................................1 Crystallography............................................................................................................................

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials & Design

سال: 2022

ISSN: ['1873-4197', '0264-1275']

DOI: https://doi.org/10.1016/j.matdes.2022.111421