Growth of Gallium Nitride Films on Multilayer Graphene Template Using Plasma-Enhanced Atomic Layer Deposition

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Template-Based Synthesis of Aluminum Nitride Hollow Nanofibers Via Plasma-Enhanced Atomic Layer Deposition

Aluminum nitride (AlN) hollow nanofibers were synthesized via plasma-enhanced atomic layer deposition using sacrificial electrospun polymeric nanofiber templates having different average fiber diameters (~70, ~330, and ~740 nm). Depositions were carried out at 200°C using trimethylaluminum and ammonia precursors. AlN-coated nanofibers were calcined subsequently at 500°C for 2 h to remove the sa...

متن کامل

Large-scale synthesis of uniform hexagonal boron nitride films by plasma-enhanced atomic layer deposition

Hexagonal boron nitride (h-BN) has been previously manufactured using mechanical exfoliation and chemical vapor deposition methods, which make the large-scale synthesis of uniform h-BN very challenging. In this study, we produced highly uniform and scalable h-BN films by plasma-enhanced atomic layer deposition, which were characterized by various techniques including atomic force microscopy, tr...

متن کامل

Ultrathin oxide films by atomic layer deposition on graphene.

In this paper, a method is presented to create and characterize mechanically robust, free-standing, ultrathin, oxide films with controlled, nanometer-scale thickness using atomic layer deposition (ALD) on graphene. Aluminum oxide films were deposited onto suspended graphene membranes using ALD. Subsequent etching of the graphene left pure aluminum oxide films only a few atoms in thickness. A pr...

متن کامل

Introduction to (plasma-enhanced) atomic layer deposition

Film growth by the atomic layer deposition (ALD) method relies on alternate pulsing of the precursor gases and vapors into a vacuum chamber and their subsequent chemisorption on the substrate surface (Fig. 1) [1,2]. The different steps in the process are saturative such that ALD film growth is self-limiting yielding one submonolayer of film per deposition cycle. ALD has some unique characterist...

متن کامل

Direct Growth of Al2O3 on Black Phosphorus by Plasma-Enhanced Atomic Layer Deposition

Growing high-quality and uniform dielectric on black phosphorus is challenging since it is easy to react with O2 or H2O in ambient. In this work, we have directly grown Al2O3 on BP using plasma-enhanced atomic layer deposition (PEALD). The surface roughness of BP with covered Al2O3 film can reduce significantly, which is due to the removal of oxidized bubble in BP surface by oxygen plasma. It w...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Acta Metallurgica Sinica (English Letters)

سال: 2019

ISSN: 1006-7191,2194-1289

DOI: 10.1007/s40195-019-00938-8