Gating System Design Solutions for Casting Defects from Pouring

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Gating Design Optimization for Improvement in Yield of Casting

Casting has many process variations depending upon the material, the type of pattern, mould and the pouring technique like sand casting, investment casting, die casting, squeeze casting and lost foam casting. Sand casting is the most widely used process which can be used to produce intricate parts in almost every metal that can be melted. Casting defects analysis is process of finding the root ...

متن کامل

Optimization of Pouring Velocity for Aluminium Gravity Casting

In current casting factories, tilting type automatic pouring machines are often used to pour the molten metal into the mold, with the operator relying on experience, perception and repeated testing to manually determine the pouring velocity. However, seeking an optimum multistep pouring velocity through trial and error results in an enormous number of combinations and is very difficult. For thi...

متن کامل

Solutions of diffusion equation for point defects

An analytical solution of the equation describing diffusion of intrinsic point defects in semiconductor crystals has been obtained for a one-dimensional finite-length domain with the Robin-type boundary conditions. The distributions of point defects for different migration lengths of defects have been calculated. The exact analytical solution was used to verify the approximate numerical solutio...

متن کامل

Aided Runner and Gating System Design from

important activities of die-casting die design. In normal practice, determine therunner and gating designparameters. These parameters are simulations on a computer and dry runs on adie-casting machine These iterative activities increase the manufacturing lead time and makes A system which could reduce the iterations and make the presentsa computer-aided system for runner and gating system gener...

متن کامل

simulation and design of electronic processing circuit for restaurants e-procurement system

the poor orientation of the restaurants toward the information technology has yet many unsolved issues in regards to the customers. one of these problems which lead the appeal list of later, and have a negative impact on the prestige of the restaurant is the case when the later does not respond on time to the customers’ needs, and which causes their dissatisfaction. this issue is really sensiti...

15 صفحه اول

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید