Galvanic Corrosion between Alloy 690 and Magnetite in Alkaline Aqueous Solutions
نویسندگان
چکیده
منابع مشابه
Galvanic Corrosion between Alloy 690 and Magnetite in Alkaline Aqueous Solutions
The galvanic corrosion behavior of Alloy 690 coupled with magnetite has been investigated in an alkaline solution at 30 °C and 60 °C using a potentiodynamic polarization method and a zero resistance ammeter. The positive current values were recorded in the galvanic couple and the corrosion potential of Alloy 690 was relatively lower. These results indicate that Alloy 690 behaves as the anode of...
متن کاملEffect of Hydrogen on Corrosion and Stress Corrosion Cracking of AZ91 Alloy in Aqueous Solutions
The effect of hydrogen on the corrosion and stress corrosion cracking of the magnesium AZ91 alloy has been investigated in aqueous solutions. Hydrogen produced by corrosion in water diffuses into, and reacts with the Mg matrix to form hydride. Some of the hydrogen accumulates at hydride/Mg matrix (or secondary phase) interfaces as a consequence of slow hydride formation and the incompatibility ...
متن کاملIs galvanic corrosion between titanium alloy and stainless steel spinal implants a clinical concern?
BACKGROUND CONTEXT Surgeons are hesitant to mix components made of differing metal classes for fear of galvanic corrosion complications. However, in vitro studies have failed to show a significant potential for galvanic corrosion between titanium and stainless steel, the two primary metallic alloys used for spinal implants. Galvanic corrosion resulting from metal mixing has not been described i...
متن کاملGalvanic corrosion between orthodontic wires and brackets in fluoride mouthwashes.
The aim of this investigation was to determine the influence of fluoride in certain mouthwashes on the risk of corrosion through galvanic coupling of orthodontic wires and brackets. Two titanium alloy wires, nickel-titanium (NiTi) and copper-nickel-titanium (CuNiTi), and the three most commonly used brackets, titanium (Ti), iron-chromium-nickel (FeCrNi) and cobalt-chromium (CoCr), were tested i...
متن کاملPhotoionization of Indole in Alkaline Aqueous Solutions
The photoionization process of indole in alkaline aqueous solutions at 77 °K and the recombination process of trapped electron with its mother molecule were investigated. The fluorescence spectrum of indole in these glassy media depended on the NaOH concentration; the disappearance of the 325 nm band at the NaOH concentrations higher than 5 M with the appearance of a fluorescence band at 375 nm...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Metals
سال: 2015
ISSN: 2075-4701
DOI: 10.3390/met5042372