Fractography of Hot Forging Die Steels

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Enhancement of hot forging die life using different methods

Forging dies at high temperatures are under contact pressure, variable mechanical loads and thermal shock, furthermore they should withstand wear and friction in a high level. So, in order to increase die life, the selection of die material, coating and hardness is essential. In this review, various methods used for die life enhancement such as carbide coating, using the super alloy stellite 6 ...

متن کامل

Estimation of Spray Lubrication and Die Temperature for Die Wear Life Prediction in Hot Forging

We have been developing a process design CAE system to predict die wear life in the process design stage for the hot forging of steel. Our goal is to reduce production costs by shortening the development period, while maximizing the life of the die. In our system, we use an expression that defines the relationship between die wear, die strength, and friction factors, such as die pressure, slidi...

متن کامل

Selection of Die Materials and Surface Treatments for Increasing Die Life in Hot and Warm Forging

In warm and hot forging, the dies are subjected to high contact pressures and temperatures. The selection of the die material, hardness and coating is critical for increasing die life. Recent studies indicate that ceramic dies and various surface treatment techniques represent, in certain applications, cost effective techniques for improving die life. This paper reviews the state of technology ...

متن کامل

Numerical Simulation of Hot Closed Die Forging of a Low Carbon Steel Coupled with Microstructure Evolution

Hot closed die forging is a regular process applied to manufacture metallic components used in supporting and fixing cable conductors in electric power transmission lines. In this forming process, the final microstructure of the workpiece depends on the control of several processing parameters. In this study, simulation of the industrial forging process of a ball hook component was performed us...

متن کامل

Determination of Load and Strain-Stress Distributions in Hot Closed Die Forging Using the Plasticine Modeling Technique

An axisymmetric hot closed die-forging process has been studied by physical modeling technique using the plasticine. To observe the material flow pattern, layers of plasticine with different colors were used. The normal direction to the layers was considered a principal direction. The strain distribution was obtained by measuring the thickness of the plasticine layers. Based on the strain distr...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Society of Materials Science, Japan

سال: 1980

ISSN: 1880-7488,0514-5163

DOI: 10.2472/jsms.29.599