Fractography of Fatigue Fracture Surface in Silumin Subjected to Electron-Beam Processing

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fatigue Fracture Characteristics of Ti6Al4V Subjected to Ultrasonic Nanocrystal Surface Modification

The influence of ultrasonic nanocrystal surface modification (UNSM) on the fatigue fracture characteristics of Ti6Al4V was investigated. Two groups of specimens were separated due to different heat treatment conditions. Group one was stress-relief annealed at 650 ◦C, and group two was then treated with solid solution-aging. UNSM with the conditions of a static load of 25 N, vibration amplitude ...

متن کامل

Tensile properties and fatigue behavior of AHSS-DP 350/600 subjected to laser shock processing

This work presents the effects of strain rate on the tensile properties and fracture morphologies of AHSS-DP 350/600 subjected to LSP. Fatigue crack growth test was performed to evaluate fatigue behavior in the metallic plate of AHSS-DP350/600. However, this material is used in automobile industry and enhancing it fatigue resistance is a challenge in material engineering. In order to evaluate a...

متن کامل

MULTI FRACTURE/DELAMINATION ANALYSIS OF COMPOSITES SUBJECTED TO IMPACT LOADINGS

A combined finite/ discrete element method is presented for modelling of composite specimens subjected to dynamic/impact loadings. The main task is set on developing an algorithm for simulation of potential bonding and debonding/delamination phenomena during impact or general dynamic loading conditions. In addition, full fracture analysis can also be performed. The proposed approach adopts a ge...

متن کامل

Fatigue Failure and Damage Analysis of an Anti-roll Bar Subjected to Fatigue Experiments

The available fatigue theories have been examined using simple specimens subjected to bending or tension-compression loads. Therefore, the stress fields have been generally one or two dimensional. Anti-roll bar is a component belongs to the suspension system of the vehicles. In spite of having simple circular section, due to the having several curvatures, this component experiences a three-dime...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: IOP Conference Series: Materials Science and Engineering

سال: 2016

ISSN: 1757-8981,1757-899X

DOI: 10.1088/1757-899x/142/1/012080