Fractographic Studies of Plastic-embedded Cells by Scanning Electron Microscopy

Three-dimensional views of cell structures at high magnifications made possible by the scanning electron microscope (SEM) are becoming increasingly useful to biologists. Methods that have proved useful for stabilizing biological soft tissue for observation in the SEM include the critical point method (1, 2), freeze drying, freeze fracturing followed by freeze drying (4, 9, 10), observation of s...

متن کامل

Fractographic failure analysis of a Procera AllCeram crown using stereo and scanning electron microscopy.

OBJECTIVES Presentation of a methodological approach using stereo and scanning electron microscope examination for the failure analysis of an alumina all-ceramic premolar crown (Procera AllCeram). METHODS The recovered part of a fractured Procera alumina crown was examined utilizing first a stereomicroscope and second a scanning electron microscope (SEM). The stereomicroscope analysis was per...

متن کامل

Observed by Scanning Electron Microscopy

The strain of P. aeruginosa used was a Fisher serotype 3,7, originally isolated from a patient with severe burns. The susceptibility of the strain to antibiotics used singly and in combination was determined by the tube dilution method (12). Minimal inhibitory concentrations (MICs) were determined by observing the lowest dilution of antibiotic that prevented visible growth of an inoculum of 105...

متن کامل

Fat uptake evaluation in fried fish fillet by using Scanning Electron Microscopy (SEM)

The aim of this study was to investigate the effects of breading materials and two different frying oils on the fat up-take in the fish fillets during frying process. Breaded and non-breaded black pomfret (Parastromateus niger) fillets were fried in sunflower oil and palm olein. Fat content by Soxhelet method and scanning electron microscopy (SEM) was studied. Results from Soxhelet method showe...

متن کامل

Examination of Lung Parenchyma by Electron Microscopy

In this paper many of the principal struc­ture of the Moral Lung were studied with the help of Electron Microscopy. Detailed descrip­tion was given of Granular Pneumocytes, Membranous Pneumocytes, Macrophages, and Alveolar Capillaries. A discussion followed on the form and function of Granular Pneumo­cytes.  Acknowledgements  I am grateful to the Reza Shah Pahlavi Foundation for its generou...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Cell Biology

سال: 1973

ISSN: 1540-8140,0021-9525

DOI: 10.1083/jcb.56.3.876