Corrosion Resistance of the Superhydrophobic Mg(OH)2/Mg-Al Layered Double Hydroxide Coatings on Magnesium Alloys
Coatings of the Mg(OH)2/Mg-Al layered double hydroxide (LDH) composite were formed by a combined co-precipitation method and hydrothermal process on the AZ31 alloy substrate in alkaline condition. Subsequently, a superhydrophobic surface was successfully constructed to modify the composite coatings on the AZ31 alloy substrate using stearic acid. The characteristics of the composite coatings wer...
متن کاملAdsorptive desulfurization of oil derivatives using nanostructured Mg-Al layered double hydroxides: Experimental design and modeling
This study focuses on the application of nanostructured Mg-Al layered double hydroxide as a promising adsorbent in desulfurization of dibenzothiophene, an aromatic sulfur bearing compound from gasoil model. The Mg-Al LDH was synthesized by a co-precipitation method and characterized by FT-IR, XRD, EDX and SEM. The XRD and FT-IR approved the layered structure and crystalline form of the adsorben...
متن کاملAdsorptive desulfurization of oil derivatives using nanostructured Mg-Al layered double hydroxides: Experimental design and modeling
This study focuses on the application of nanostructured Mg-Al layered double hydroxide as a promising adsorbent in desulfurization of dibenzothiophene, an aromatic sulfur bearing compound from gasoil model. The Mg-Al LDH was synthesized by a co-precipitation method and characterized by FT-IR, XRD, EDX and SEM. The XRD and FT-IR approved the layered structure and crystalline form of the adsorben...
متن کاملFRACTIONAL RECRYSTALLIZATION KINETICS IN DIRECTLY COLD ROLLED Al-Mg, Al-Mg-Sc AND Al-Mg-Sc-Zr ALLOY
The evaluation of texture as a function of recrystallization has been characterized for directly cold rolled Al-6Mg, Al-6Mg-0.4Sc and Al-6Mg-0.4Sc-0.2Zr alloys. Samples were annealed isothermally at 400 °C for 1 to 240 minutes to allow recrystallization. Recrystallization kinetics of the alloys is analyzed from the micro-hardness variation. Isothermally annealed samples of aluminum alloys were ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: DEStech Transactions on Engineering and Technology Research
سال: 2017
ISSN: 2475-885X
DOI: 10.12783/dtetr/icmme2017/9130