Exploring Infrared Sensoring for Real Time Welding Defects Monitoring in GTAW
This paper presents an evaluation of an infrared sensor for monitoring the welding pool temperature in a Gas Tungsten Arc Welding (GTAW) process. The purpose of the study is to develop a real time system control. It is known that the arc welding pool temperature is related to the weld penetration depth; therefore, by monitoring the temperature, the arc pool temperature and penetration depth are...
متن کاملA Real-Time Spectroscopic Sensor for Monitoring Laser Welding Processes
In this paper we report on the development of a sensor for real time monitoring of laser welding processes based on spectroscopic techniques. The system is based on the acquisition of the optical spectra emitted from the laser generated plasma plume and their use to implement an on-line algorithm for both the calculation of the plasma electron temperature and the analysis of the correlations be...
متن کاملOn Line Monitoring for Defects in Electric Arc Stud Welding
ABSTRACT The application of on-line monitoring system for recording main welding parameters during electric arc stud welding process at different electric arc stability changes is described in this paper. In the first part of the paper, the basics of electric arc stud welding process, and equipment for stud welding and process monitoring used in experimental part is described. In the second par...
متن کاملWelding Aluminum Alloy 6061 with Opposing Dual Torch Gtaw Process
Cracking is a major concern in welding aluminum alloys. Although weld solidification cracks can be eliminated through addition of filler alloy, the additives modify the alloy or base-metal constituents and may not always be desirable. High-energy beam processes, such as electron-beam welding, that result in minimal heat input reduce crack sensitivity, but their high cost limits their applicatio...
متن کاملReal-time human activity monitoring exploring multiple vision sensors
In this paper we describe the monitoring of human activity in an indoors environment through the use of multiple vision sensors. The system described in this paper is made up of three cameras. Two of these cameras are active and are part of a binocular system. They operate either as a set of three static cameras or as a set of one xed camera and an active binocular vision system. The human acti...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Sensors
سال: 2010
ISSN: 1424-8220
DOI: 10.3390/s100605962