Evolution of Lattice Spacing of Gamma Double Prime Precipitates During Aging of Polycrystalline Ni-Base Superalloys: An In Situ Investigation

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys

Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys R.R. Unocic a,∗, G.B. Viswanathan a, P.M. Sarosi a, S. Karthikeyan b, J. Li a, M.J. Mills a a Department of Materials Science and Engineering, The Ohio State University, 477 Watts Hall, 2041 College Road, Columbus, OH 43210, USA b Department of Materials Engineering, Indian Institute of Science Bangalore, Karnataka 5600...

متن کامل

Modeling displacive–diffusional coupled dislocation shearing of c0 precipitates in Ni-base superalloys

In Ni-base superalloys, superlattice extrinsic stacking fault (SESF) shearing of c0 precipitates involves coupled dislocation glide and atomic diffusion. A phase-field model is developed to study this process, in which the free energy of the system is formulated as a function of both displacement and long-range order parameter. The free energy surface is fitted to various fault energy data obta...

متن کامل

an investigation of accuracy and complexity across different proficiency levels in written narrative task

abstract this quasi-experimental study was aimed at examining the impact of storyline complexity on the grammatical accuracy and complexity of advanced and intermediate efl learners. a total of 65 advanced and intermediate efl learners were selected from iran language institute (ili). an intact group including 35 intermediate participants and another intact group with 30 advanced participants ...

an investigation into iranian teachers consistency and bias in evaluation of students writings

while performance-based language assessment has led to an increased authenticity and content validity in the practice of writing assessment, the reliability of ratings has become a major issue. research findings have shown different reactions by native english speaker (nes) and non-native english speaker (nns) teachers to students’ writings. the focus of this study is on investigating whether i...

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metallurgical and Materials Transactions A

سال: 2019

ISSN: 1073-5623,1543-1940

DOI: 10.1007/s11661-019-05536-y