Evaluation of Vickers Hardness by Nanoindentation Measurement.
نویسندگان
چکیده
منابع مشابه
Low-Load Vickers Microindentation Hardness Testing
ADVANCED MATERIALS & PROCESSES • APRIL 2012 I n 1925 in the UK, Smith and Sandland developed an indentation test that used a squarebased pyramidal-shaped indenter made of diamond[1]. The test was developed because the Brinell test (introduced in 1900), which (until recently) used a round hardened steel ball indenter, could not test steels harder than ~450 HB (~48 HRC). They chose this shape wit...
متن کاملBrinell and Vickers Hardness Measurement Using Image Processing and Analysis Techniques
Mechanical hardness testing is fundamental in the evaluation of the mechanical properties of metallic materials due to the fact that the hardness values allow one to determine the wear resistance of the material involved, as well as the approximate values of its ductility, flow tension, among a number of other key characteristics. As a result, the main objective of the present work has been the...
متن کاملComparative Depth of Cure Among Two Light-Cured Core Build-Up Composites By Surface Vickers Hardness
OBJECTIVE Depth of cure of composite material is restricted and it depends on many parameters such as thickness. The aim of this in-vitro study was to evaluate the depth of cure of two light-cured core build-up composites (Quixfil and Photocore) in different thicknesses, when cured for 60 seconds. MATERIALS AND METHODS The Vickers microhardness measurements were made for each side of the top ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: TRANSACTIONS OF THE JAPAN SOCIETY OF MECHANICAL ENGINEERS Series A
سال: 1998
ISSN: 0387-5008,1884-8338
DOI: 10.1299/kikaia.64.2567